1. ALEKSANDRA WÓJCIK, ADAM KRAJEWSKI, ANDRZEJ RADOMSKI:
Controlling of wood destroying anobiidae using para-dichlorobenzene in aerobic atmosphere
2. ESPOSITO CORCIONE CAROLA, FRIGIONE MARIAENRICA: Novel UV-cured
nanocomposite used for the protection of walnut wood artworks
3. AGNIESZKA JANKOWSKA, PAWEŁ KOZAKIEWICZ: Comparison of outdoor and
artificial weathering using compressive properties
4. LUIZ FERNANDO DE MOURA, DIEGO VALÉRIO BRAIDO DOS SANTOS,
JOSÉ OTÁVIO BRITO: Effect of heat treatment on color, weight loss, specific gravity and
equilibrium moisture content of two low market valued tropical woods
5. BIN NA, XIAONING LU, ANTONIO PIZZI: Creep and temperature-dependent creep of
one component polyurethane adhesives for green wood gluing
6. FRANTIŠEK HAPLA, STEPHAN KUBALEK, MIKLÓS BAK, RÓBERT
NÉMETH*: Timber grade oriented analysis of Abies grandis trees’ ovendry density with different growth
rates. Part II.: Effect of the trees’ social position in the forest on the variability of ovendry density
7. ERGUN BAYSAL *, SELIM DEGIRMENTEPE, TURKAY TURKOGLU, HILMI
TOKER: Some mechanical and physical properties of AD-KD 5 impregnated and
thermally modified scots pine wood
8. IGOR DŽINČIĆ, DRAGAN ŽIVANIĆ: The influence of fit on the distribution of glue
in oval tenon/mortise joint
9. SAMUEL AMMANN, PETER NIEMZ: Fibre and adhesive bridging at glue joints in
European beech wood
10. ERTAN ÖZEN, OSMAN GÖKTAŞ, ALI KASAL, HASAN EFE, SELÇUK
DEMIRCI: Bending moment capacity of L-type furniture corner joints constructed of particleboard
produced from vine pruning residues
11. IZABELA MODZELEWSKA, ANNA JASZCZUR: Analysis of the degree of mycological
biodegradation of ligno-cellulose material with organic filling through self-breaking estimation
and with the usage of electronic microscope
12. KENNOUCHE SALIM, ZERIZER ABDELATIF, SITOUAH NOURDINE,
AKNOUCHE ABDELHAMID, FREDERIC MOTHE: Characterization of Algerians oak
wood by X-ray tomographic scanner and free software image-j
13. CİHAT TAŞÇIOĞLU*, ÇAĞLAR AKÇAY, MESUT YALÇIN, HALİL İBRAHİM
ŞAHİN: Effects of post-treatment with Ca and CCa on screw withdrawal resistance of wood based
composites
14. HAN CHEN-JING, XU JIN-MEI, JIANG JIA-LI, JIANG JING-HUI,
LV JIAN-XIONG*: Moisture content distribution of multiple Eucalyptus veneers during
hot-press-drying
15. HASAN HÜSEYON TAŞ, MUSTAFA ALTINOK, MESUT ÇIMEN: The strength
properties changing according to type corner joints and adhesive of the wood-based furnitures under the
effect of dynamic forces
16. VASILIKI KAMPERIDOU, IOANNIS BARBOUTIS, VASILEIOS VASILEIOU:
SHORT NOTE- Influence of thermal treatment on mechanical strength of scots pine (Pinus sylvestris L.)
wood
Contents
Download WR20140200 Contents
Download WR20140201 Articles
Download WR20140202 Articles
Download WR20140203 Articles
Download WR20140204 Articles
Download WR20140205 Articles
Download WR20140206 Articles
Download WR20140207 Articles
Download WR20140208 Articles
Download WR20140209 Articles
Download WR20140210 Articles
Download WR20140211 Articles
Download WR20140212 Articles
Download WR20140213 Articles
Download WR20140214 Articles
Download WR20140215 Articles
Download WR20140216 Articles