1. LADISLAV REINPRECHT, MILOŠ PÁNEK:
Bio-treatment of spruce wood for improving of its permeability and soaking
Part 2: Direct treatment with the fungus trichoderma viride . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 1
2. BOŽENA KOŠÍKOVÁ, ELENA SLÁVIKOVÁ, FRANTIŠEK KAČÍK:
Biodegradability of extractives in sound and biologically decayed beech by various yeast species . . . 9
3. BOŠTJAN LESAR, BOŠTJAN PODLESNIK, FRANC POHLEVEN, MIHA HUMAR,
POLONA KRALJ, MARJAN VEBER:
Performance of boron-ethanolamine-quaternary ammonium based wood preservatives against
leaching, wood decay and blue stain fungi . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 17
4. OSMAN GOKTAS, ERGUN BAYSAL, ERTAN OZEN, RAMAZAN MAMMADOV,
M. EMIN DURU:
Decay resistance and color stability of wood treated with Juglans regia extract . . . . . . . . . . . . . . . . 27
5. RICHARD HRČKA, MARIAN BABIAK, ROBERT NÉMETH:
High temperature effect on diffusion coefficient . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 37
6. MARCIO ROGÉRIO DA SILVA, GILMARA DE OLIVEIRA MACHADO,
CARLITO CALIL JUNIOR, L. JAY DEINER:
Permeability measurements of brazilian Pinus elliottii . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 47
7. MÁRIA FIŠEROVÁ, JURAJ GIGAC, ŠTEFAN BOHÁČEK, MICHAL ROSENBERG:
Sugar beet pulp fibrous residues as bonding agents in papermaking . . . . . . . . . . . . . . . . . . . . . . . . . . 57
8. HÜDAVERDI EROĞLU, SEZGIN KORAY GÜLSOY:
A comparative study of some tumorous and normal hardwood kraft pulp properties . . . . . . . . . . . 77
9. TAMAS HOFMANN, T. RÉTFALVI, L. ALBERT, PETER NIEMZ:
Investigation of the chemical changes in the structure of wood thermally modified
within a nitrogen atmospehere autoclave . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 85
10. ROBERT PEPLIŃSKI, JAN DUDZIŃSKI, JERZY MAJKA:
Effects of the initial moisture content variation of beech (Fagus sylvatica l.)
Veneer on its waviness and the moisture content distribution after drying . . . . . . . . . . . . . . . . . . . . 99
11. BOJAN BUČAR, MIRAN MERHAR:
Modelling of response of aerodynamic excited idling circular saw blade with
geometrical imperfection . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 111
12. NATALIYA ANISIMOVA:
Simulation and directing measures in wood utilization . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 121
Download WR200803 00 Contents
Download WR200803 01 Articles
Download WR200803 02 Articles
Download WR200803 03 Articles
Download WR200803 04 Articles
Download WR200803 05 Articles
Download WR200803 06 Articles
Download WR200803 07 Articles
Download WR200803 08 Articles
Download WR200803 09 Articles
Download WR200803 10 Articles
Download WR200803 11 Articles
Download WR200803 12 Articles