Wood density and annual ring width of pedunculate oak from stands grown on former agricultural land

The main aim of this study was to determine differences in basic density and average annual ring width of pendulate oak wood collected from trees grown on former agricultural land and on forest land, using a dimensional method. The experiment was carried out in the western part of Poland, near to Poznan, which is in the central part of the European range of pedunculate oak. In our study the average basic density was 0.528 g.cm-3, and the value for former agricultural land was lower by 0.026 g.cm-3 than that for forest land. Differences in basic density values between these two land types were statistically significant. The average annual ring width in samples collected from forest land in our study was 2.48 mm, samples from former agricultural land were characterized by wider average annual rings. The results suggest that there are significant differences in quality of wood from former agricultural land and from forest. However, from view of wood quality and applications the difference is not important.

The gradient of wood moisture within-stem of sessile oak (Quercus petraea (matt.) Liebl.) in summer

In the xylem of growing trees water fills both free spaces in the cell walls and capillary spaces. For this reason its share in the tree mass is very high. As a result transport of logs obtained from fresh-felled trees is mainly equivalent to the transport of contained water. The primary aim of this study was to determine wood moisture content in growing trees in the selected season of the year. Absolute moisture content of tested wood was established at 62.4%. Average moisture content in heartwood was 60.6% and it was lower by approx. 6% from moisture content in sapwood. Moisture content of the oak heartwood is high, similar to central part of the trunk of non – heartwood species. It is an exceptional situation in comparison to heartwood species, particularly conifers.

Variations of wood properties of birch (Betula pendula Roth) from a 23-year old seed orchard

This work presents the results of selected wood properties in birch trees grown on a provenance experiment plot established as a seed orchard. The study concerned: basic density, oven-dry density and compression strength along the grain at a moisture content of 0% and at moisture content above fiber saturation point. Analyses were performed on 971 wood samples collected from 28 trees at the level of breast height. It was found high variability for diameter of breast height (22%) and relatively low for basic density (9%) and oven-dry density (11%). Average basic density was 446.5 kg.m-3 and average oven-dry density was 537.9 kg.m-3. The compression strength at 0% moisture content was four times higher (65 MPa) than the strength at moisture content above the fiber saturation point (16.6 MPa). Most of clones had similar properties within the limits of statistical errors, but a few clones exhibited statistically significant low value.

Biosocial diversity of scots pine (pinus sylvestris l.) in a tree stand in relation to chosen hydraulic conductivity indicators of the stem

The research focused in determining the lignification indicator of fresh needled springs and the mass of fresh needles in reference to the lignin content in tracheid walls of peripheral area of the stem (MFT/LC and MFN/LC) of Scots pine differentiated as far as its biosocial position within the community expressed by Kraft’s classification. The material for the analysis came from mature pine stands growing on North European Plain, on the territory of Poland. Chemical and structural analyses of wood encompassed the area of mature sapwood, i.e. thickness of the last 10 annual rings located at 1.3 m (DBH). It seems that the noticed differences values of both indicators (MFT/LC and MFN/LC) in pines belonging to the first three Kraft’s biological classes are connected with physiological, physical and structural conditionings of water transport with minerals in xylem and are closely connected with competition for sunlight, water, nutrients and living space.