Ratio analysis between compression and shearing of 72 Brazilian wood species

The Brazilian standard ABNT NBR 7190 (1997) governs the premises for the wood structure sizing through a table and the simplified method. Thus, this research aims to analyze whether the simplified method shown in the standard matches the resistance values of 72 Brazilian species, separated from class C20 to C60. In the end, it was possible to conclude that the value displayed by the standard between the ratio of shear and compression in the direction parallel to the fibers is half of what actually happens in Brazilian species, showing an urgent review in the standard premises.

Physical and mechanical characterization of Planchonella Pachycarpa wood species for use in structural purpose

This research aimed to characterize the wood species Goiabão (Planchonella pachycarpa), following the precepts set forth in the Brazilian standard ABNT NBR 7190, as well as to evaluate the possibility of estimating physical and mechanical properties, using the analysis of variance (ANOVA) as a function of apparent density, and also to estimate the stiffness properties as a function of the respective strength property. The physical and mechanical properties were considered adequate for the use of this wood for structural purposes, being classified in class C40. According to the results of the regression models, it is possible to estimate the tensile strength parallel to the fibers as a function of the apparent density. It was also possible to estimate the longitudinal elastic modulus in the compression parallel to the fibers as a function of the compressive strength parallel to the fibers.