Segment of wall panel for timber structures under vertical load

The subject of this paper is an experimental and numerical analysis of the stability of the wall panels with one-side board sheathing for timber structures. The reinforcement of the panel is provided using glued timber composite I-shaped element consisting of a web made of a wood-based desk embedded into flanges of solid timber. The mechanism of the behaviour of these panels, mode of the failure and reliable procedure to determine the buckling load-bearing capacity not been fully explored so far. This work describes the behaviour of the wall panel under vertical load and the method of failure using experimental and numerical analysis. The reduction coefficient kJ was determined, which can be used for a simple calculation of the buckling capacity of a wall panel.

Correlations and differences between methods for non-destructive evaluation of timber elements

The aim of this paper is to compare the results of evaluation of mechanical properties of timber by visual assessment, two grading machines, three devices for measuring in-situ and destructive tests. The most important result is the comparison of static and dynamic modulus of elasticity of timber, and further comparison of strength classes obtained by different measuring methods.