Anatomical properties of straw of various annual plants used for the production of wood panels

The aim of this study was to determine basic anatomical features of annual plant fibers used as wood substitutes for the production of wood-based panels. For this purpose rye, wheat, triticale, rape and corn straw were used. The determination of the morphological features of the fibers was conducted on the macerated material. Fiber lengths, fiber diameters and lumens were measured, and then the fiber wall thicknesses and slenderness ratios were calculated. The result clearly showed significant differences among all fiber characteristics of the tested plants. The strength and direction of the relationship between the anatomical properties determined in the study and the physicomechanical properties of the boards produced with straw from the tested annual plants were identified.

The soy flour as an extender for uf and muf adhesives in birch plywood production

Formaldehyde emission still remains a major disadvantage of widely applied formaldehyde-containing amino resins such as UF (urea-formaldehyde) resin and MUF (melamine-urea-formaldehyde) resin. The compositions of adhesives for plywood manufacturing have to contain a proper extenders in order to adjust their viscosity. Thus, the aim of the study was to investigate the effect of protein-rich soy flour (SF) as the extender for adhesives. The composition of flours and their ability to absorb the formaldehyde were determined. Properties of liquid resins such as gel time, viscosity, pH and solid content were investigated. The possible chemical interaction between the extenders and resins were assessed with the use of FTIR spectroscopy. Plywood panels manufactured using UF and MUF adhesives with the soy flour introduced as the extender in various concentrations were tested in terms of shear strength and formaldehyde release. Studies have shown that soy flour has a favorable composition and formaldehyde-scavenging ability. The addition of SF affected resins properties such as viscosity and gel time but showed no influence on their pH and solid content. FTIR analysis has not explained the chemical interaction between resin and extender. The application of soy flour in the concentration of 15% for UF resin and 10% for MUF resin allowed to produce plywood characterized by improved bonding quality and decreased formaldehyde emission.