Authors
-
Xianwu Zhou
Chinese Academy of Forestry, Research Institute of Wood Industry, Beijing, China
-
Yurong Wang
Chinese Academy of Forestry, Research Institute of Wood Industry, Beijing, China
-
Li Wang
Chinese Academy of Forestry, Research Institute of Wood Industry, Beijing, China
-
Jianxiong Lv
Chinese Academy of Forestry, Research Institute of Wood Industry, Beijing, China
-
Rongjun Zhao
Chinese Academy of Forestry, Research Institute of Wood Industry, Beijing, China
-
Lihong Yao
Inner Mongolia Agricultural University, College of Material Science and Art Design, Hohhot, China
-
Zhangjing Chen
Northwest A&F University, P. R. China Virginia Tech University, USA