Model construction and microwave preheating experiments using fiberboard

Authors

  • Chunmei Yang

    Northeast Forestry University, China

  • Zanbin Zhu

    Northeast Forestry University, China
    Xinyang Agriculture and Forestry University, China

  • Jiuqing Liu

    Northeast Forestry University, China

  • Bo Xue

    Northeast Forestry University, China

  • Yucheng Li

    Northeast Forestry University, China

Post Views: 87
Posted in WOOD RESEARCH Volume 68, Number 2, 2023Tagged Comsol, fiberboard, microwave, thermal radiation

Search for a Keyword

Cite This Article

YANG, CH., ZHU, Z., LIU, J., XUE, B & LI, Y. (2023): Model construction and microwave preheating experiments using fiberboard. In: Wood Research 68 (2), 389-402 pp., available at: doi.org/10.37763/wr.1336-4561/68.2.389402

Articles in this Release

  • Evolution and distribution of shakes in larch logs during air…

  • Discoloration of oak veneer induced by metal ions

  • Chemical composition and potential uses of Leucaena leucocephala stem bark

  • Water retention of beech shavings heat-treated at lower temperatures

  • A synergic effect of water-based acrylic resin with boric acid…

  • Quality of beech, birch and oak wood from stands growing…

  • Response surface optimization based on freeze-thaw cycle pretreatment of poplar…

  • Prediction of efficacy of deacidification process

  • Fixation of dye-type red and blue ink handwriting on aged…

  • Determination of mode I fracture properties of European spruce

  • Effects of Pyrolysis process on products yield of plywood from…

  • Volatile organic compounds and metals adsorption capacity of wood bark-based…

  • Optimization of the manufacturing of Metasequoia-based three-layer structure parquet flooring…

  • Model construction and microwave preheating experiments using fiberboard

  • Short notes: First report of the lignivorous fungus Paecilomyces maximus…

Copyright © 2023 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)