Properties of the water-resistant plywood glued with pf resin with the addition of tannin filler and nanoclay

Authors

  • Dorota Dukarska

    Poznan University of Life Sciences, Poznan, Poland

  • Jakub Kawalerczyk

    Poznań University of Life Sciences, Poland

  • JUSTYNA WŁODARCZYK

    Poznan University of Life Sciences, Poznan, Poland

Post Views: 192
Posted in WOOD RESEARCH Volume 67, Number 2, 2022Tagged filler, Nanoclay, phenol-formaldehyde adhesive, Plywood

Search for a Keyword

Cite This Article

DUKARSKA, D., KAWALERCZYK, J. & WLODARCZYK, J. (2022): Properties of the water-resistant plywood glued with pf resin with the addition of tannin filler and nanoclay. In: Wood Research 67 (2), 241-253 pp., available at: doi.org/10.37763/wr.1336-4561/67.2.241253

Articles in this Release

  • The relationship between bulk density and thermal conductivity in various…

  • Seasonal dynamic changes of sapwood and heartwood in larix gmelinii

  • Decay resistance of preservative injected poplar and its process of…

  • Enhancing leucaena leucocephala wood preservation by steeping it in boron…

  • Effects of differrent boron-based flame retardants on the combustibility of…

  • Analysis of moisture content variation on strength and stiffness properties…

  • Properties of the water-resistant plywood glued with pf resin with…

  • Modelling a clt specimen protected with gypsum exposed to parametric…

  • Study on flame retardant leach resistant of modified poplar wood

  • Determination of mode I fracture behavior of southern yellow pine…

  • Design and performance of nail connection in wood framing shear…

  • Effect of wood flour content on the properties of flat…

  • The tactile perception evaluation of wood surface with different roughness…

  • Study on thermal comfort of wood tabletop materials

  • Methods of preparation of nanofibrillated cellulose for special filter papers…

Copyright © 2023 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)