Relationship between cell lumen area and lignin content of alkaline-treated densified timber of Paraserianthes falcataria

Authors

  • Vinodini Raman

    Universiti Malaysia Sabah, Malaysia

  • Kang Chiang Liew

    Universiti Malaysia Sabah, Malaysia

  • Rafidah Md Salim

    Universiti Malaysia Sabah, Malaysia

Post Views: 164
Posted in WOOD RESEARCH Volume 67, Number 3, 2022Tagged alkaline pretreatment, densification, low-density timber, Paraserianthes falcataria, scanning electron microscopy

Search for a Keyword

Cite This Article

RAMAN, V., LIEW, K. CH. & SALIM, R. M. (2022): Relationship between cell lumen area and lignin content of alkaline-treated densified timber of Paraserianthes falcataria. In: Wood Research 67 (3), 393-401 pp., available at: doi.org/10.37763/wr.1336-4561/67.3.393401

Articles in this Release

  • Impact of heat treatment on the surface color and glossiness…

  • Effect of UV radiation on change in color of steamed…

  • Why the sound-absorbing performance of heartwood and sapwood differs in…

  • Comprehensive evaluation of hawthorn wood characteristics in relation to soil…

  • Relationship between cell lumen area and lignin content of alkaline-treated…

  • Timbre harmonic of selected hardwood species

  • Effects of fire retardants on mechanical properties and water resistance…

  • Modelling of steel to timber joint exposed to fire

  • Steam-pressing mechanism of low density magnesia-bonded wood-wool panel

  • Deformation behavior of circular saw blades with different body structures…

  • Modelling of post–consumer wood sorting and manipulation: Computational conception and…

  • A micro-graph retrieval system for coniferous woods using multiple methods

  • Bamboo defect classification based on improved transformer network

  • Short notes: A research on the application of industrial by-product…

Copyright © 2023 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)