Effect of acid hydrolyses on properties of cellulose/poly furfural alcohol (PFA) composites from maize stalk

The study investigated morphology and thermal properties of cellulose/poly furfural alcohol (PFA) composites prepared from maize stalk through acid mixtures. The cellulose nanocrystals (CNCs) were extracted from maize stalk via acid hydrolysis using mixtures of various acids. The prepared CNCs were encapsulated in a PFA matrix via in situ polymerization process using p-toluene sulfonic acid as catalyst. The properties of untreated maize stalk, cellulose and their nanocomposites were analysed by scanning electron microscope (SEM), X-ray diffraction (XRD), Fourier transmission infrared (FTIR) and thermogravimetric analysis (TGA). The crystallinity of maize stalk was generally increased after an acid hydrolysis dominated by H2SO4/HNO3 and H2SO4/HCl. The same trend was observed from TGA, except that H2SO4/H3PO4 and H2SO4/HClO4 dominated thermal stability trailed by H2SO4 hydrolysed CNC nanocomposite. The surface breakage of fibers observed in SEM images was depended on the strength of acids used to hydrolysed the CNC. There was also evidence of aggregation and cracked PFA surface with addition of acid hydrolysed CNCs, dependent on the acids strength. The H2SO4/HClO4 hydrolysed CNC/PFA displayed a fairly good dispersion of CNCs in the PFA matrix with no surface breakage.

Effect of H2SO4/HCLO4 mixture on properties of sugarcane bagasse cellulose crystals

The main objective of the study was to investigate the effect of mixed acid concentration on the morphology, crystallinity and thermal properties of cellulose nanocrystals (CNCs). Acid hydrolysis using mixture of sulphuric (H2SO4) acid and perchloric (HClO4) acid was used to extract CNCs from sugarcane bagasse (SCB). The properties of the raw SCB, extracted cellulose, 45% H2SO4 hydrolysed CNCs, 45% H2SO4/HClO4 hydrolysed CNCs, 55% H2SO4/HClO4 hydrolysed CNCs and 65% H2SO4/HClO4 hydrolysed CNCs were analysed using Fourier transmission infrared spectroscopy (FTIR), X-ray diffraction (XRD), scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). The crystallinity of SCB was significantly increased after bleaching and acid hydrolysis. Acid hydrolysis using 55% H2SO4/HClO4 showed the highest crystallinity. The TGA results showed significant increase in thermal stability of 55% H2SO4/HClO4. The lowest thermal stability was observed with 45% H2SO4 hydrolysed CNCs. The order of thermal stability was raw SCB < extracted cellulose < 45% H2SO4 hydrolysed CNCs < 65% H2SO4/HClO4 hydrolysed CNCs < 45% H2SO4/HClO4 hydrolysed CNCs < 55% H2SO4/HClO4 hydrolysed CNCs. The SEM results showed fibre breakage for 65% H2SO4/HClO4 hydrolysed CNCs. The fibre breakage seemed to be acid concentration dependent.