Permeability and mechanical behaviour of microwave pre-treated Norway spruce ripewood

This is a study of the influence of microwave (MW) pre-treatment on the permeability of Norway spruce ripewood (Picea abies L. Karst) as it affects its mechanical properties. Specimens were treated under variable moisture content, MW intensity, and impregnation processes. According to the results, the specimens with an initial moisture content of 45–65% exhibited the highest permeability values compared to reference samples. An insignificant difference was found between MW pre-treatments at 2 and 3 kW. Statistically significant results were found after long-time (24h) vacuum-pressure impregnation (LP). The average retention value following LP was 132 kg.m-3, which is almost three times greater than the MW-treated groups impregnated in a short-time vacuum-pressure process. The average depth of penetration after LP was 2.0 mm and the proportion of the impregnation area following LP was 17.6%. MW pre-treatment had no effect on the impregnability or the mechanical properties of the wood; other MW regimes are open for further examination.

Effect of different pre-treatments on the permeability of glue-laminated bamboo

In this study, hydrothermal treatments (duration: 2 h, 5 h, 8 h; temperature: 60°C, 80°C, 100°C), ultrasonic treatments (duration: 60 min, 90 min, 120 min; temperature: 40°C, 50°C, 60°C; ultrasonic power: 400 W, 600 W, 800 W) and freeze-drying treatments (vacuum degree: 0.05 mbar, 0.1 mbar, 0.5 mbar, 1.0 mbar, 1.7 mbar) were performed respectively to improve the permeability of glue-laminated bamboo. The effects of different pre-treatments on the permeability were compared according to the water absorption test and the mercury intrusion porosimetry test. The microstructure change of the samples was observed by scanning electron microscope (SEM). The results showed that freeze-drying treatment was an effective way to increase the permeability of the samples, in which the water absorption rate can be increased by 47%, and the porosity can be increased by 10% at 0.5 mbar vacuum. From SEM analysis, some small holes appeared in the cell wall of the freeze-dried samples, because he free water inside the samples was changed into ice, and the volume became larger, and the pore diameter of the bamboo was enlarged.