{"id":3799,"date":"2021-09-24T09:00:12","date_gmt":"2021-09-24T07:00:12","guid":{"rendered":"http:\/\/www.woodresearch.sk\/cms\/?p=3799"},"modified":"2021-09-24T09:00:32","modified_gmt":"2021-09-24T07:00:32","slug":"experimental-tests-of-timber-connections-with-glued-in-rods-in-bending","status":"publish","type":"post","link":"https:\/\/www.woodresearch.sk\/cms\/experimental-tests-of-timber-connections-with-glued-in-rods-in-bending\/","title":{"rendered":"Experimental tests of timber connections with glued-in rods in bending"},"content":{"rendered":"\n<div class=\"wp-block-pdf-viewer-block-standard\" style=\"text-align:left\"><div class=\"uploaded-pdf\"><a href=\"https:\/\/www.woodresearch.sk\/cms\/wp-content\/uploads\/2021\/09\/Experimental-tests-of-timber-connections-with-glued-in-rods-in-bending.pdf\" data-width=\"\" data-height=\"\"><\/a><\/div><\/div>\n","protected":false},"excerpt":{"rendered":"<p>The article deals with research of joints with glued-in threaded rods. The introduction provides a brief presentation of the issue. The first part focuses on axially loaded glued-in threaded rods. The second part explains the behaviour of joints with glued-in rods loaded by bending moment. Theoretical analysis was performed on models based on the finite element method. Verification of theoretical results was realized by practical experiments. Tensile tests were carried out on timber blocks with glued-in bars to verify the depth of affixing. Furthermore, the resistance in bending was confirmed on actual beams with glued-in bars in the middle of the span. Results and the follow-up work are summarized in the conclusion.<\/p>\n","protected":false},"author":4,"featured_media":0,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[412],"tags":[3463,3462,3461,2262,1282,245],"release_year":[],"ppma_author":[3300,3301,3302,3303,3304,2333,3305],"class_list":["post-3799","post","type-post","status-publish","format-standard","hentry","category-wood-research-volume-61-number-4-2016","tag-epoxy","tag-glued-in-rods","tag-polyurethane","tag-rotation","tag-timber","tag-wood"],"featured_image_src":null,"author_info":{"display_name":"Maro\u0161 Kov\u00e1\u010d","author_link":"https:\/\/www.woodresearch.sk\/cms\/author\/kovacvupc-sk\/"},"authors":[{"term_id":3300,"user_id":0,"is_guest":1,"slug":"vladimir-duchon","display_name":"Vladim\u00edr Ducho\u0148","avatar_url":"https:\/\/secure.gravatar.com\/avatar\/?s=96&d=mm&r=g","0":null,"1":"","2":"","3":"","4":"","5":"","6":"","7":"","8":""},{"term_id":3301,"user_id":0,"is_guest":1,"slug":"tomas-klas","display_name":"TOM\u00c1\u0160 KLAS","avatar_url":"https:\/\/secure.gravatar.com\/avatar\/?s=96&d=mm&r=g","0":null,"1":"","2":"","3":"","4":"","5":"","6":"","7":"","8":""},{"term_id":3302,"user_id":0,"is_guest":1,"slug":"orsolya-katona","display_name":"Orsolya Katona","avatar_url":"https:\/\/secure.gravatar.com\/avatar\/?s=96&d=mm&r=g","0":null,"1":"","2":"","3":"","4":"","5":"","6":"","7":"","8":""},{"term_id":3303,"user_id":0,"is_guest":1,"slug":"jan-brodniansky","display_name":"J\u00c1N BRODNIANSKY","avatar_url":"https:\/\/secure.gravatar.com\/avatar\/?s=96&d=mm&r=g","0":null,"1":"","2":"","3":"","4":"","5":"","6":"","7":"","8":""},{"term_id":3304,"user_id":0,"is_guest":1,"slug":"lubos-balcierak","display_name":"\u013dubo\u0161 Balcier\u00e1k","avatar_url":"https:\/\/secure.gravatar.com\/avatar\/?s=96&d=mm&r=g","0":null,"1":"","2":"","3":"","4":"","5":"","6":"","7":"","8":""},{"term_id":2333,"user_id":0,"is_guest":1,"slug":"jaroslav-sandanus","display_name":"Jaroslav Sandanus","avatar_url":"https:\/\/secure.gravatar.com\/avatar\/?s=96&d=mm&r=g","0":null,"1":"","2":"","3":"","4":"","5":"","6":"","7":"","8":""},{"term_id":3305,"user_id":0,"is_guest":1,"slug":"kristian-sogel-2","display_name":"Kristian S\u00f3gel","avatar_url":"https:\/\/secure.gravatar.com\/avatar\/?s=96&d=mm&r=g","0":null,"1":"","2":"","3":"","4":"","5":"","6":"","7":"","8":""}],"_links":{"self":[{"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/posts\/3799","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/users\/4"}],"replies":[{"embeddable":true,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/comments?post=3799"}],"version-history":[{"count":2,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/posts\/3799\/revisions"}],"predecessor-version":[{"id":3802,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/posts\/3799\/revisions\/3802"}],"wp:attachment":[{"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/media?parent=3799"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/categories?post=3799"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/tags?post=3799"},{"taxonomy":"release_year","embeddable":true,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/release_year?post=3799"},{"taxonomy":"author","embeddable":true,"href":"https:\/\/www.woodresearch.sk\/cms\/wp-json\/wp\/v2\/ppma_author?post=3799"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}