Thermogravimetric analysis, differential scanning calorimetry and time-to-ignition of wood materials treated with water glass flame retardants

Authors

  • Juraj Jancík

    University of Zilina, Slovakia

  • Linda Makovická Osvaldová

    University of Žilina, Slovakia

  • Frank Markert

    Technical University of Denmark, Denmark

Post Views: 180
Posted in WOOD RESEARCH Volume 66, Number 1, 2021Tagged cone calorimetry, fibreboard, mass loss, pyrolysis, Simultaneous thermal analysis, spruce, time of ignition

Search for a Keyword

Cite This Article

JANCIK, J., MAKOVICKA OSVALDOVA, L. & MARKERT, F. (2021): Thermogravimetric analysis, differential scanning calorimetry and time-to-ignition of wood materials treated with water glass flame retardants. In: Wood Research 66 (1), 15-26 pp., available at: doi.org/10.37763/wr.1336-4561/66.1.1526

Articles in this Release

  • Wood species identification based on an ensemble of deep convolution…

  • Thermogravimetric analysis, differential scanning calorimetry and time-to-ignition of wood materials…

  • Experimental and numerical studies on mechanical behaviors of beech wood…

  • The concentration of selected heavy metals in poplar wood biomass…

  • Study on the structure and properties of poly(3-hydroxybutyrate-co-4-hydroxybutyrate)/ rubber wood…

  • Antioxidant activity of Swietenia macrophylla king bark extracts

  • Comparison of thermal transfer and inkjet printing of UHF RFID…

  • Effect of silica on alkaline bagasse cellulose and softwood cellulose

  • Effects of light thermal treatments on the color, hygroscopity and…

  • Cross-correlation of color and acidity of wet beech wood in…

  • Wood properties comparation of Cedrela odorata from trees in agroforestry…

  • Effect of hot pressing modification on surface properties of rubberwood…

  • Study on lamb wave propagation characteristics along the grain of…

  • Analysis of cutting force in the process of chipless felling…

  • Synthesis and characterization of resol type phenol-formaldehyde resin improved by…

Copyright © 2025 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)