Effect of corrugated board structure on mechanical properties

Authors

  • Włodzimierz Szewczyk

    Lodz University of Technology,
    Poland

  • Maria Bieńkowska

    Lodz University of Technology,
    Poland

Post Views: 364
Posted in WOOD RESEARCH Volume 65, Number 4, 2020Tagged board base, Corrugated board, corrugated board strength, flute height

Search for a Keyword

Cite This Article

SZEWCZYK, W. & BIENKOWSKA, M. (2020): Effect of corrugated board structure on mechanical properties. In: Wood Research 65 (4), 653-662 pp., available at: doi.org/10.37763/wr.1336-4561/65.4.653662

Articles in this Release

  • The physiological and biochemical mechanisms of Cinnamomum camphora xylem extracts…

  • Wood quality of six eucalyptus clones planted in northern Mato…

  • A calibration method of the laser triangular measuring system to…

  • Analysis of tracheid morphological characteristics, annual rings width and latewood…

  • Effect of steam explosion on enzymatic hydrolysis of various parts…

  • Leachability of ACQ-D after three different preservative treatments

  • CLT construction performance under thermal loading

  • Study on the permeation and fixation of ACQ-C in poplar

  • Investigation of urea usage in soda pulping of Populus deltoides

  • Effect of heat treatment on the surface color of rubber…

  • Prestress losses in spruce timber

  • Effect of corrugated board structure on mechanical properties

  • Emission of volatile camphor compounds from Cinnamomum camphora wood

  • Evaluation of corner joint strength of composite panels bonded with…

  • Short note: The impact of glue-lines on the protective effect…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}