Study on sanding force, power consumption and quality of calibrating sanding recombinant bamboo

Authors

  • Beijing Forestry University, College of Materials Science and Technology,
    Beijing, P. R. China

  • Beijing Forestry University, College of Materials Science and Technology,
    Beijing, P. R. China

  • Beijing Forestry University, College of Materials Science and Technology,
    Beijing, P. R. China

  • Beijing Forestry University, College of Materials Science and Technology,
    Beijing, P. R. China

  • Beijing Forestry University, College of Materials Science and Technology,
    Beijing, P. R. China

  • Beijing Forestry University, College of Materials Science and Technology,
    Beijing, P. R. China

  • Beijing Forestry University, College of Materials Science and Technology,
    Beijing, P. R. China