Study of dewatering characteristics of eucalyptus wood by supercritical CO2

Authors

  • HONGHAI LIU

    NANJING FORESTRY UNIVERSITY, PEOPLE’S REPUBLIC OF CHINA

  • XIAOKAI ZHANG

    Nanjing Forestry University, China

  • Jingwen Zhang

    Nanjing Forestry University, China

Post Views: 724
Posted in WOOD RESEARCH Volume 67, Number 6, 2022Tagged characteristics, deformation, dewatering, Eucalyptus wood, supercritical CO2

Search for a Keyword

Cite This Article

Liu, H., Zhang, X. & Zhang, J. (2022): Study of dewatering characteristics of eucalyptus wood by supercritical CO2. In: Wood Research 67 (6), 908-918 pp., available at: doi.org/10.37763/wr.1336-4561/67.6.908918

Articles in this Release

  • Impact of temperature and ultraviolet radiation on changes of colour…

  • Study of dewatering characteristics of eucalyptus wood by supercritical CO2

  • Evaluation of wood surface roughness by confocal microscopy

  • Effect of H2SO4/HCLO4 mixture on properties of sugarcane bagasse cellulose…

  • Fire retardant performance of sugi and hinoki treated with phosphorus…

  • Intensification of the freeze-thaw pretreatment of disintegrated poplar wood

  • Study on the dispersion characteristics of wood acoustic emission signal…

  • Modelling for single-wall corrugated fibreboard with a trapezoidal core under…

  • Influence of wood species on quality of exterior transparent acrylic…

  • Experimental verification of the modern semi-rigid timber connections

  • Dimensional stability and durability of hybrid sandwich panel made from…

  • Study on machining properties and surface coating properties of heat…

  • Research progress of solid wood bending softening technology. Review

  • Comparative study on physical-mechanical properties of plywood produced from eucalyptus…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}