Skip to content
Wood Research
Menu
  • Home
  • Author guidelines
  • Journal Issues
  • Contact

THE EFFECT OF SUPPORT LAYER MATERIAL AND ADHESIVE TYPE ON COMPRESSIVE DYNAMIC BENDING AND SHEAR STRENGTH IN LAMINATED WOOD

Authors

  • HILAL ULAŞAN

    GAZI UNIVERSITY, TURKEY

  • CEVDET SÖĞÜTLÜ

    GAZI UNIVERSITY, TURKEY

Post Views: 1,537
Posted in WOOD RESEARCH Volume 69, Number 3, 2024Tagged compressive strength, dynamic bending, lamination, reinforcement, shear strength, Wood

Search for a Keyword

Cite This Article

ULAŞAN, H., SÖĞÜTLÜ, C. (2024): The effect of Support Layer Material and adhesive type on Compressive Dynamic Bending and Shear Strength in laminated wood. In: Wood Research 69 (3), 402-416 pp., available at: doi.org/10.37763/wr.1336-4561/69.3.402416

Articles in this Release

  • EFFECT OF PHENOL FORMALDEHYDE RESIN IMPREGNATION ON NANODYNAMIC VISCOELASTICITY OF…

  • OPTIMIZING THE AMOUNT OF FLAME RETARDANT USED FOR SPRUCE WOOD

  • THE INVESTIGATION OF NATURAL AGING BEHAVIOR OF SOME WOOD SPECIES…

  • PREPARATION PROCESS AND INTERFACE MODIFICATION ON THE MECHANICAL PROPERTIES OF…

  • IMPACT OF HOLLOW CORE DIAMETER AND BFRP WRAPPING ON AXIAL…

  • DETERMINATION OF FLEXURAL STRENGTH AND YOUNG’S MODULUS OF ELASTICITY OF…

  • FLEXURAL STRENGTHENING OF THERMALLY MODIFIED RUBBERWOOD GLULAM BEAMS WITH FRP…

  • THE X-BAND MICROWAVE ABSORPTION CHARACTERISTICS OF POROUS ACTIVATED CARBON FROM…

  • FRACTURE MECHANISM ANALYSIS OF HIGH-DENSITY FIBREBOARD BASED ON DIGITAL IMAGE…

  • A METHOD OF SIMULATING SEAT LOAD FOR NUMERICAL ANALYSIS OF…

  • EVALUATION OF PROPERTIES OF WOOD PLASTIC COMPOSITES MADE FROM SEVEN…

  • THE EFFECT OF SUPPORT LAYER MATERIAL AND ADHESIVE TYPE ON…

  • CHANGES IN WOOD QUALITY OF BETULA ERMANII LOGS BY HEATING…

  • STUDY OF STRESS WAVE PROPAGATION PATH AND DEPTH IDENTIFICATION IN…

  • EXPERIMENTAL TESTS OF RED MERANTI (SHOREA SPP.) DOWEL BEARING STRENGTH…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}