PREPARATION AND PERFORMANCE OF ANTI MILDEW GLUED LAMINATED BAMBOO
In order to strengthen the anti-mildew and anti-aging properties of bamboo when exposed outdoors, the glued laminated bamboo was impregnated with four different kinds of anti-mildew agents: tebuconazole, 3-Iodo-2-propargyl butyl carbamate (IPBC), NaBF4/didecyl dimethyl ammonium chloride (DDAC), boric acid/borax, and waterborne polyurethane coatings modified with boric acid/borax and triazole (UV1130), nano-TiO2 and nano-SiO2 were coated respectively. The modified coated glued laminated bamboo was characterized and analyzed through the experiments of wear resistance, three-point bending resistance and mildew resistance. The results showed that the glued laminated bamboo impregnated with 0.5% NaBF4/DDAC, and then coated with the waterborne polyurethane modified with boric acid/borax and nano TiO2 (the mass ratio:7.5/7.5/1.0) possessed the best mildew resistance, mechanical properties and weather resistance