Comparative Surface Roughness Evolution of 33 Japanese Hardwoods after Water and Fire-Retardant Treatments Using 3D Optical Profilometry

In this study, we assessed the surface roughness of 33 Japanese hardwood species by 3D optical profilometry (ISO 25178) and examined the influence of water and fire-retardant treatments. The surface roughness on cross, radial, and tangential sections was evaluated using the arithmetic mean height (Sa) parameter. Measurements were performed on untreated samples and repeated on the same spots after water treatment and NF300 fire-retardant treatment. Surface roughness varied widely across species and anatomical sections and tended to decrease with increasing wood density. The surface roughness increased with both treatments compared to the untreated wood. The maximum increase was on tangential surfaces after NF300 treatment, where the mean Sa value increased from 30.14 ± 17.05 μm to 42.05 ± 19.60 μm (39.5%). The statistical analysis showed a significant difference between the untreated and NF300-treated tangential surfaces (p = 0.011).

Short notes. INFLUENCE OF WOOD ANATOMY ON THE DISTRIBUTION OF GUANIDINE BASED FIRE RETARDANTS IN FIVE FAST GROWING JAPANESE HARDWOODS

This study investigates the influence of wood anatomy on the distribution of fire retardant chemicals in five fast-growing Japanese hardwood species (Melia azedarach, Toona sinensis, Choerospondias axillaris, Alnus japonica, and Liriodendron tulipifera). Given Japan’s increasing demand for sustainable and locally sourced materials, fire retardant treatments are critical for enhancing fire resistance in fast-growing hardwoods used for construction. Using low vacuum scanning electron microscopy (SEM), we examined the distribution of fire retardants in cross-section, radial section, and tangential sections, comparing the effectiveness in ring-porous versus diffuse-porous species. Results revealed that diffuse-porous species (Alnus japonica and Liriodendron tulipifera) retained higher levels of fire retardants with a more even distribution. In contrast, ring-porous species (Melia azedarach, Toona sinensis, Choerospondias axillaris) showed the highest chemical concentration at the edges.

EFFECTS OF HOLE PERFORATION AND SURFACE CUTTING ON WOOD ELASTICITY USING ULTRASONIC AND VIBRATION METHODS

This study analyzed how hole perforation and surface cutting affect ultrasonic wave propagation velocity and resonant frequency in wood. While non-destructive evaluation techniques for wood elasticity are well-established, the specific influence of defects like holes and orthogonal cuts on wave behavior remains underexplored. This study aimed to fill this gap by assessing how these defects influence wave behavior and providing new insights into their impact on wood’s mechanical properties. Four softwood species and seven hardwood species were analyzed. In hardwood specimens, ultrasonic propagation velocity and resonant frequency were measured under increasing levels of hole perforation (9, 27, and 45 holes). In contrast, the effects of one and two orthogonal surface cuts were examined in softwood specimens. The results revealed that the ultrasonic propagation velocity decreased noticeably with an increasing number of holes. Meanwhile, resonant frequency exhibited only a slight decrease. In contrast, softwoods displayed minimal changes in ultrasonic velocity but notable reductions in resonant frequency due to surface cutting. This study highlights the differences in continuous wave propagation pathways associated with the two defect types and estimation methods, offering novel insights into wood evaluation techniques

EFFECTS OF CHEMICAL AND PHYSICAL TREATMENTS ON BAMBOO CELL WALL STRUCTURE FROM ENGINEERING PERSPECTIVES

This study focuses on the effects of chemical treatment using polyethylene glycol (PEG) and physical treatment via steam explosion and microwave, with a comprehensive analysis using ATR-FTIR, X-ray diffraction, Keyence VR 6000 optical profilometer, and SEM. The aim is to elucidate alterations in bamboo cell walls following these treatments compared to untreated bamboo. The results reveal significant modifications in the chemical composition and crystalline structure of bamboo cell walls post-treatment. ATR-FTIR analysis indicates changes in functional groups, suggesting chemical interactions and modifications in the molecular arrangement of cell wall components. XRD analysis further corroborates these findings by revealing shifts in crystallinity and peak intensities, signifying structural rearrangements, as evidenced by optical images and SEM micrographs

Relationship between Wood Anatomical Features and Surface Roughness Characteristics

This study aimed to investigate the relationship between surface roughness and anatomical features of wood in 15 different species of boards. Surface roughness was measured parallel and perpendicular to the wood grain using a surface profilometer, and anatomical features such as pore size and distribution were analyzed using microscopic techniques. The results showed that surface roughness perpendicular to the grain direction was consistently higher than that parallel to the grain direction for all wood samples. This difference in roughness was correlated with pore size and density. It shows that the larger pores and lower density lead to higher roughness perpendicular to the grain. The study also found that traditional hand planning methods (push and pull) produced a smooth surface finish, with no statistical differences in roughness.

Short notes: Can the physical properties of wood samples be predicted from photographs displayed on a monitor?

This study focused on evaluating the physical properties of wood from photographs displayed on a monitor. Sample photos of 475 hardwoods and their physical information were collected from a wood database. R, G, and B values were extracted from the wood photos using color picker software. Statistical techniques such as Pearson’s correlation coefficient and multiple regression analysis were applied to investigate relationships between wood color and physical properties. From results of Pearson’s correlation coefficient, R, G, and B values were most affected by specific gravity. In a multiple regression analysis, tree size, specific gravity, and modulus of rupture (MOR) were significant in the positive (+) direction by color (R, G, and B). On the other hand, modulus of elasticity (MOE) was significant in the negative (-) direction at the 1% level by color. The specific gravity of wood had the most significant effect on R, G, and B values in multiple regression analysis. In conclusion, the color and specific gravity of wood were related closely. Additionally, it is possible to predict the physical properties of wood from the R, G, and B values of a wood sample photograph displayed on a monitor. These results could provide useful information for wood researchers as well as wood exporters and importers.

Investigation on the Malaysian Duabanga moluccana cross sections as sound absorbing functional materials

This study focused on Duabanga moluccana, which is a fast-growing tropical tree native to Southeast Asia. Duabanga moluccana cross sectional specimens were analyzed to gas permeability, pore size, and open-pore porosity and also measured its sound absorption coefficients with an impedance tube. Duabanga moluccana showed a larger pore size and greater open-pore porosity than other hardwood species, and its sound absorbing performance was superior to that of the gypsum board currently used as a commercial ceiling material. Although this was a laboratory-scale investigation, we demonstrate that Duabanga moluccana cross sections have potential as a natural sound absorbing functional building material.

Why the sound-absorbing performance of heartwood and sapwood differs in yellow poplar (Liriodendron tulipifera) cross-sections?

In this study, we investigated why the sound-absorbing performance is different with between heartwood and sapwood of yellow poplar, which are known for their sound-absorbing properties. We performed image observation as well as gas permeability, pore size, and porosity analysis, and measured the sound absorption coefficient of all samples using an impedance tube. We determined that the pores were significantly larger, and the gas permeability and through-pore porosity much higher, in the sapwood than the heartwood. The average sound absorption coefficient of the sapwood at 2000-6400 Hz (0.61 ± 0.04) was 2.7x that of the heartwood (0.23 ± 0.03). The average NRC of the sapwood (0.23 ± 0.01) was 1.9x that of the heartwood (0.12 ± 0.01). This study ultimately determined that the sapwood, as a consequence of its larger pore size and superior through-pore porosity, which thereby improved its gas permeability, outperformed the heartwood in terms of sound-absorption. We also determined that pore size and through-pore porosity were the primary parameters that determined the sound-absorbing performance of yellow poplar cross-sections.

The relationship between bulk density and thermal conductivity in various korean woods

The article deals with the effects of bulk density on thermal conductivity in specimens of 15 Korean woods (Zelkova serrata, Pinus densiflora, Cornus controversa, Betula schmidtii, Betula platyphylla var. japonica, Ginkgo biloba L., Cedrela sinensis A. Juss., Fraxinus mandshurica, Ulmus davidiana var. japonica, Prunus sargentii Rehder, Paulownia tomentosa (Thunb.) Steud., Larix kaempferi (Lamb.) Carrière, Robinia pseudoacacia, Kalopanax septemlobus and Tilia amurensis). The results of this study were compared with previous studies performed on wood specimens from China, India, and Turkey. Consistent with these previous studies, bulk density and thermal conductivity were positively correlated in Korean woods, and a simple regression model with a very high correlation of R2 (94%) was obtained. Interestingly, we observed some variation between our simple regression models and those generated by previous researchers who had examined non-Korean woods.