THE EFFECTS OF INTERFACIAL MODIFICATIONS ON THE PROPERTIES OF BAMBOO FIBER /WASTE TETRA PAK /PLA COMPOSITES

In this study, BF/TP/PLA ternary composite was constructed utilizing bamboo fiber (BF) as the reinforcing phase and waste Tetra Pak (TP) along with polylactic acid (PLA) as the matrix. The effects of different interfacial modification methods on the properties of the composites were systematically investigated. Bamboo fibers were modified using a silane coupling agent (KH570), nano-SiO2, and compatibilizers (MAH-g-PLA, MAH-g-PE). The composites were subsequently fabricated via hot pressing, and their mechanical properties, water absorption, chemical structure, and micromorphology were characterized. The results showed that after KH570 treatment, the flexural modulus and flexural strength of the composites increased by 15% and 32%, respectively. Following the introduction of compatibilizers, the water absorption was further reduced, and the thickness swelling rate was significantly improved. Optimal comprehensive performance was achieved at a nano-SiO2 content of 1 wt%; the flexural modulus reached 2524.1 MPa, exceeding the requirement of Chinese standard LY/T 3275-2021 for outdoor wood-plastic composites (≥2500 MPa), while the water absorption decreased to its lowest value (11.3%). Furthermore, interfacial bonding became more compact.

THE EFFECTS OF INTERFACE MODIFICATION ON THE PROPERTIES OF WASTE WOOD/POLYBUTYLENE SUCCINATE COMPOSITES

In this study, wood-plastic composites were prepared using waste wood powder (WWP) and polybutylene succinate (PBS). Three interfacial modifiers, γ-glycidoxy-propyltrimethoxysilane (KH560), isopropyl tri(dioctylpyrophosphate) titanate (CS201), and maleic anhydride-grafted PBS (MAPBS) were used to modify the interface of the composites and enhance the mechanical properties. The materials were characterized using infrared spectroscopy, three-point bending, and water absorption tests. The results indicated that all three interfacial modifiers were successfully grafted onto the wood powder surface, thereby influencing the mechanical properties. When the mechanical properties of the composites reached their optimal levels, the optimal loading levels of KH560, CS201, and MAPBS were 2%, 1%, and 2%, resp. At this point, compared to the unmodified composite, the elastic modulus increased by 9.44%, 15.03%, and 12.92%, resp; the flexural strength increased by 5.35%, 11.51%, and 8.91%, resp; the water absorption decreased by 4.88%, 3.68%, and 6.21%, resp; and the thickness swelling decreased by 4.56%, 3.08%, and 7.54%, resp.

WEATHERABILITY OF BAMBOO/PPC COMPOSITES MODIFIED WITH IPBC/DDAC AND UV1130

In this study, a compound anti-mold agent IPBC/DDAC and an ultraviolet absorber UV1130 were used to enhance the weatherability of bamboo/polypropylene carbonate (PPC) composites exposed outdoors. The samples were evaluated by mechanical test, surface color difference analysis, anti-ageing test and mold resistance test. The results indicated that the appropriate addition of IPBC/DDAC and UV1130 effectively mitigated the decline in tensile strength and flexural strength caused by changes in environmental factors; however, their impact on the variation in impact strength was not as significant. At the same level of IPBC/DDAC modification, the higher contents of the UV1130 introduction into the composites, the better surface color stability could be obtained. The introduction of appropriate amount of IPBC/DDAC and UV1130 can effectively improve the mold resistance, water vapor and thermal resistance of bamboo/PPC composite, in which the water vapor resistant level could be up to Grade 5, and no obvious cracks or bubbling were observed on the surface of the composites; the anti-mold efficiency of the composites could be above 90%

EFFECTS OF WASTE POLYETHYLENE ON THE PROPERTIES OF BAMBOO/POLYPROPYLENE CARBONATE COMPOSITES

Bamboo-plastic composites were made by bamboo fibers (BF), polypropylene carbonate (PPC) and waste polyethylene (PE), modified with 3-iodo-2-propargyl butyl carbamate/didecyldimethyl ammonium chloride (IPBC/DDAC) as fungicides and UV1130 as ultraviolet absorbent to prolong their service life for outdoor application, in which 10%, 20%, 30%, 40% and 50% of PPC were replaced by waste PE, respectively to reduce their cost. The modified composites were characterized and analyzed by mechanical properties test, surface color difference analysis, and mold resistance test. The results showed that the tensile strength, bending strength and impact strength of BF/PPC/waste PE composites would decrease as the waste PE content increased, and only when the waste PE content was not higher than 20%, the mechanical properties could meet the application requirements for indoors and outdoors. The introduction of IPBC/DDAC and UV1130 could take positive effects on the mechanical properties, surface color stability and mold resistance of BF/PPC composites, while the tensile strength, bending strength and impact strength of BF/PPC/PE composites were 2.36%, 1.85%, and 1.67% lower than the modified BF/PPC composites, as well as the values of ∆L*, ∆a*, and ∆b* of the composites were lower , and the value of ∆E was higher than the BF/PPC modified composites after three months of outdoor exposure. The efficacy levels of the modified BF/PPC and BF/PPC/waste PE composites could be increased to 98.8% and 56.75%, respectively, due to the excellent mold resistance of the combined antifungal agents of IPBC/DDAC