The Study on the Frequency Response Characteristics of Wood Orthotropy Based on Stress Wave Propagation Direction and Distance

This study investigates the frequency response of Zelkova schneideriana and Pinus sylvestris var. mongholica Litv. along longitudinal, radial, and tangential directions at different propagation distances. Sinusoidal signals from 20 to 200 kHz with 2 kHz intervals were applied using a piezoelectric device, and the responses were recorded by an acoustic emission sensor. Frequency response curves were obtained from the amplitude ratios of response to excitation signals. The results showed that attenuation in the radial direction was lower than that in the longitudinal and tangential directions between 20 and 100 kHz. Both species exhibited stable characteristic response bands around 35, 154, and 188 kHz, which showed good agreement with one-dimensional elastic wave theory, with a minimum relative error of 0.48%. Zelkova schneideriana also exhibited a characteristic frequency near 79 kHz and more stable high-frequency responses.

THE STUDY ON THE DAMAGE CHARACTERISTICS OF PINUS SYLVESTRIS VAR. MONGOLICA UNDER DIFFERENT MOISTURE CONTENTS

This study investigated the effects of moisture content (0%, 12%, 20%, 30%, 40%, 50%) on the mechanical behaviour and damage evolution of Pinus sylvestris var. mongolica three-point bending tests. A Weibull distribution model quantified damage progression, extracting scale (λ) and shape (k) parameters. Results revealed moisture regulated failure mechanisms, Low moisture (≤20%) induced brittle fracture (high k, low λ) with tensile crack dominance and stress concentration. High moisture (≥30%) promoted ductility (low k, high λ) via enhanced λ, driven by shear cracks. Mixed cracks persisted across all stages. Moisture altered cell wall plasticization, inter-fibre friction, and interfacial bonding, modulating damage evolution. Weibull modelling effectively captured stage dependent damage variable trends. Increased moisture facilitated fibre slippage and interlayer shear through lubrication and cell wall softening.This work establishes quantitative links between moisture content, mechanical response, and micromechanical damage mechanisms in wood, providing insights for moisture dependent structural applications of engineered timber.

Research on clustering identification of acoustic emission events in the process of wood crack propagation using PCA

This study presents a methodology for feature extraction and identification of acoustic emission (AE) events during wood crack propagation utilizing Principal component analysis (PCA) and enhanced K-means clustering algorithm. Experimental setups included double cantilever beam (DCB) for mode I crack propagation analysis and three-point bending test for mixed-mode crack propagation assessment. Various AE parameters, such as amplitude, duration, absolute mean value, peak frequency, and frequency centroid, were computed. PCA applied for dimensionality reduction to extract principal components and eliminate redundant information. The optimal number of clusters was determined using a combination of the elbow method and the Davies-Bouldin index to classify damage modes. Results indicate that the principal components contribute to 88.5% and 92% of the variance in the two tests, respectively, yielding three distinct types of AE events in both crack propagation scenarios. Specifically, high-frequency, low-amplitude signals correspond to microcrack initiation; low-frequency, low-amplitude signals signify interface delamination; and high-amplitude, long-duration events indicate mode I opening macroscopic damage (high frequency) and mixed-mode macroscopic failure (low frequency).

THE ANISOTROPIC VELOCITY MODEL OF INTERNAL ACOUSTIC EMISSION SIGNALS IN ZELKOVA WOOD AND THE INFLUENCE OF HOLES ON THEIR PROPAGATION PROCESS

In this article, an acoustic emission (AE) source was generated through pencil-lead break (PLB). On Zelkova schneideriana specimens featuring central through-holes with diameters ranging from 8 to 16 mm, the time-difference-of-arrival (TDOA) in combination with the least squares fitting approach was utilized to establish an anisotropic model of the AE wave velocity within the wood as it varies with the detection angle. Then, a pulse signal was generated through a signal generator to analyze the influence of the holes on the peak values of AE signals at different angles. The results indicate that when the propagation angle is less than 80°, the AE wave velocity rises rapidly with the increase of the angle and eventually approximates the longitudinal wave velocity along the grain. The AE signal peak emerged in the direction approximately 30° for the specimen without holes. In the presence of holes, as the hole diameter increases, the variation trend of AE peak amplitudes within an angular range of -18° to +18° relative to the hole center becomes progressively smoother, with a concurrent reduction in their mean value. This distinct characteristic can serve as a robust indicator for identifying internal hole defects in wood

ANISOTROPIC PROPAGATION CHARACTERISTICS OF ACOUSTIC EMISSION SIGNALS IN WOOD

This study investigates the propagation characteristics of acoustic emission (AE) signals in Zelkova schneideriana and Pinus sylvestris var. mongolic along different directions, with a focus on amplitude and frequency variations. Sinusoidal signals ranging from 10 to 400 kHz, along with pulsed signals of 1 μs width and 1 s period, were generated using an arbitrary waveform generator to simulate the AE source. Experiments were conducted on 80 mm cubic wood specimens, with the AE source and sensors positioned at the geometric centers of each surface. AE signals were recorded at a sampling rate of 2 MHz. The results indicate that, at the same frequency, the Zelkova schneideriana exhibits higher signal amplitude and energy than the Pinus sylvestris var. mongolic. Frequency response analysis further reveals that wood enhances the propagation of signals below 75 kHz, while significantly attenuating signals above 200 kHz in the transverse direction

RESEARCH ON WOOD DAMAGE FRACTURE CHARACTERISTICS BASED ON ACOUSTIC EMISSION RA-AF VALUE AND ENERGY CONCENTRATION

To study the acoustic emission (AE) characteristics and fracture properties of wood at different stress stages, three-point bending tests and real-time AE monitoring were carried out on Zelkova schneideriana and Pinus sylvestris var. in this paper. Different stress stages were classified according to AE ringing counts-cumulative AE ringing counts-load curves, damage modes of wood at different stages were identified based on distribution characteristics of RA-AF data, and fracture behavior of wood was predicted by energy concentration k. Results show that distribution characteristics of AE RA-AF data can characterize the types of cracks generated in each stress stage of wood. The crack modes generated by both specimens during three-point bending loading are tension shear composite cracks, and the proportion of tensile cracks is significantly higher than that of shear cracks, but during the elastic-plastic stage, Zelkova schneideriana specimens will produce a large number of shear cracks, whereas Pinus sylvestris var. specimens have predominantly tensile cracks, with only a small number of shear cracks produced before and after fracture. The sudden change in the energy concentration k curve between elastic-plastic deformation stage and fracture stage can be used as a precursor of damage for both specimens under three-point bending test conditions

ANISOTROPIC VELOCITY MODEL AND ENERGY ATTENUATION CHARACTERISTICS OF ACOUSTIC EMISSION SIGNALS IN FINGER-JOINTED TIMBER AND SAWN TIMBER

Although anisotropic propagation behavior of acoustic emission (AE) in the sawn timber (ST) has been revealed, that in finger-jointed timber (FJT) is still less known.Therefore, a series of velocity and energy models of AE signalswere built as it propagates along different directions on the surface and inside of specimens (ST and FJT). At first, using polar coordinate system, velocity model in 36 directions was built in FJT, which was compared to ST.Furthermore, a continuous sine wave with a frequency of 165 kHz was selected as AE source to explore the energy attenuation law in FJT and ST respectively.The results showed that there are significant differences in velocity models between FJT and ST.The wavefront in STwas regular elliptical, while that in FJT has a clear depression in perpendicular to grain direction.This feature becomes more obvious with the increase of distance when AE signal propagates inside the FJT.Inside the FJT,energy magnitude in STwas 3.00-7.37 times of that in FJT

STUDY OF STRESS WAVE PROPAGATION PATH AND DEPTH IDENTIFICATION IN CRACKED WOOD BASED ON ACOUSTIC EMISSION AND COMSOLSIMULATION

The propagation velocity models were built using AE sensors to capture stress wave on pine specimen surface.On the different specimens, cracks were made in different numbers and the depth was gradually increased from 0 mm to 90 mm at 10 mm intervals. AE experiment was combined with COMSOL to investigate propagation path.The results show that R-squared is 0.996 when fitting tangent of angle to propagation velocity.At smaller crack depths, stress wave is diffracted around crack tip and then continues to propagate in to sensor along a straight line.However, as the crack depth increases, the reflected wave at the end face will arrive at the detection location faster with significantly weaker diffraction.The area with dimensions of20×10 mm was identified about the crack tip by crack identification method

EVALUATION OF WOOD DAMAGE AND FRACTURE BEHAVIOR BASED ON ENERGY ENTROPY OF ACOUSTIC EMISSION SIGNALS

In order to assess the damage and fracture behavior of wood under continuous loading, an energy entropy and b-value associated with the acoustic emission (AE) signal were defined to quantitatively describe the release of strain energy during loading. Firstly, the acoustic emission signals of the wood in the three-point bending test were collected. This paper presents the concept of energy entropy according to the definition of information entropy. In order to further evaluate the strain energy intensity released by the damage behavior of the wood specimen, the acoustic emission b-value was defined. Finally, by jointly analysing the dynamics of these two parameters, the test process can be divided into three phases. The results show that even in the elastic phase, micro-destructive behavior occur inside the wood specimen; in the plastic phase, the wood specimen is not only subjected to macroscopic damage, but also often accompanied by fine cracks inside

Study on Acoustic Black Hole Effect of Acoustic Emission Signals in Pinus sylvestris var. mongolica litv

The difference in density and wave velocity causes distinct wave impedance between air and wood, resulting in complex acoustic emission (AE) signals due to reflection on the wood’s surface. This study explores the suppression of AE signal reflection by modifying the structure of thin wood panels, utilizing the theory of acoustic black holes (ABH). Initially, a one-dimensional ABH structure was created by forming a wedge structure on one side of the specimen. Pencil-lead break (PLB) tests simulated sudden AE sources on the specimen’s surface. AE signals were collected using three equidistant sensors on the upper surface, with a sampling frequency of 2 MHz. The AE signal was then segmented into frequency bands using the differential method and analyzed in both time and frequency domains. Comparisons were made to understand the impact of the one-dimensional ABH on AE signal propagation. Results demonstrated that the one-dimensional ABH effectively suppressed AE signal reflection on the wood’s surface, reducing the high-frequency components by 18.31%, 20.83%, and 12.09% for each sensor, respectively. Furthermore, the experimental cut-off frequency of 0.98 kHz surpassed the theoretically calculated value of 0.39 kHz due to the disparity between the ABH structure’s thickness and the theoretical prediction.

Experimental analysis of acoustic emission propagation velocities and energy attenuation law of p and s waves in wood using improved TDOA measurements

To explore the propagation law of AE signal in wood, the propagation velocity of P-wave and S-wave and the energy attenuation law of different frequency components were studied By PLB (pencil-lead break) tests. Firstly, an improved time-difference-of-arrival (TDOA) method was designed to determine the arrive time. The propagation velocities of P-wave and S-wave were calculated. Then, the Young’s modulus was estimated by P-wave velocity. Finally, on the basis of eliminating the influence of standing wave, the energy attenuation models were obtained by numerical fitting and wavelet decomposition. The results showed that the improved TDOA algorithm can calculate the propagation velocity of P-wave and S-wave at the same time through one test, and the P-wave velocity can be used to estimate the Young’s modulus. P-wave propagated faster in soft wood, while S-wave propagated faster in hard wood. The higher the frequency of AE signal, the faster the energy attenuation.

Study on the dispersion characteristics of wood acoustic emission signal based on wavelet decomposition

Artificial AE sources were generated on the surfaces of Ulmus pumila, Zelkova schneideriana, Cunninghamia lanceolata, and Pinus sylvestris var. mongolica Litv. specimens. The AE transverse wave signal was decomposed into 3-layers detail signals by wavelet decomposition and reconstructed, and it was calculated based on correlation analysis. Then the longitudinal wave speed was calculated according to the time-difference-of-arrival (TDOA) method, and the wood dispersion phenomenon was studied. The results showed that the dispersion phenomenon of Ulmus pumila was obvious. The propagation speed of high-frequency signal was 2.38 times that of low-frequency signal. The ratio of high and low frequency propagation speed of soft wood was 1.72 and 1.73. The dispersion degree of Zelkova schneideriana was the weakest, and the propagation speed of the high frequency was 1.25 times of the low one. The ratios of longitudinal and transverse wave speeds of the four specimens were 4.59, 4.07, 4.24 and 4.2, respectively.

Research on the effect of wood surface cracks on propagation characteristics and energy attenuation of longitudinal acoustic emission

To investigate the effect of Zelkova schneideriana surface cracks on the longitudinal wave propagation characteristics of acoustic emission (AE). Different sizes and numbers of cracks were made on the surface of the specimen, the propagation characteristics of AE longitudinal waves along wood texture direction were studied. Firstly, five regular cracks with the same length, different width, depth and equidistant distribution were fabricated on the surface of the specimen. The burst and continuous AE sources were generated by lead core breakage and signal generator, and the AE signals were acquired by 5 sensors with sampling frequency was set to 500 kHz. Then, the propagation speed of AE longitudinal wave was calculated by Time Difference of Arrival (TDOA) based on lead core breakage. Finally, the 150 kHz pulse signals of different voltage levels generated by the signal generator were used as AE sources to study the influence of cracks on the attenuation of AE longitudinal wave energy. The results showed that the AE longitudinal wave propagation speed under the crack-free specimen was 4838.7 m.s-1. However, after the regular crack was artificially made, the longitudinal wave speed reduced to a certain extent, and the relative error of the change was not more than 9%. Compared with the energy decay rate of 1.29 in the crack-free specimen, the decay rate gradually increased to 2.08 with the increase of the crack cross-sectional area.

Study on the time-frequency characteristics and propagation law of acoustic emission longitudinal waves in wood grain direction

To study the propagation law of acoustic emission (AE) longitudinal waves in wood, the relationship among wave velocity, standing wave fundamental frequency and Young’s modulus of elasticity was studied, and the energy decay model of AE longitudinal waves along the grain direction was established. Firstly, the propagation velocity of the longitudinal wave was calculated using the time-difference method. Then, the relationship between the wave velocity and Young’s modulus of elasticity was analyzed and the method of calculating the longitudinal wave velocity using the fundamental frequency was proposed. Finally, using different levels’ pulse strings as AE sources, the attenuation law of AE signal energy with distance was studied. The results show that the longitudinal wave velocity can be estimated more accurately by using the standing wave fundamental frequency. The influence of Poisson’s ratio needs to be considered when calculating the Young’s modulus of elasticity by using the longitudinal wave velocity.

Study on lamb wave propagation characteristics along the grain of thin wood sheet

Through the time-frequency analysis of the propagation waveform of the acoustic emission (AE) signal propagating in the thin sheet of Pinus sylvestris var. mongolica, the propagation characteristics of the stress wave when propagating as a lamb wave was studied. An AE source was generated on the surface of the specimen, the discrete wavelet transform method was used to achieve AE signal de-noising and reconstruct the waveform of the AE signal. On this basis, the time difference positioning method was used to calculate the propagation velocity of lamb waves, and compared with the propagation characteristics of lamb waves in the metal specimen. The results show that the high-frequency mode of lamb waves attenuated sharply as they propagate in the thin wood sheet, indicating that the microstructure of wood has a significant low-pass characteristic for lamb waves. The average attenuation rates of lamb waves in metal and thin wood sheet were 87.1% and 75.7%, and the velocity was 4447.0 m.s-1 and 1186.3 m.s-1, respectively. This shows that AE signals can travel longer distances in the thin wood sheet, but the propagation velocity is significantly reduced.