PREPARATION OF ECO-FRIENDLY COMPOSITE PAPER WITH GINKGO LEAF AND BIO-BASED FIBERS

Authors

  • ZIXING MA

    JIANGNAN UNIVERSITY, CHINA

  • MENG ZHOU

    JIANGNAN UNIVERSITY, CHINA

  • YANGYI WANG

    JIANGNAN UNIVERSITY, CHINA

  • QIYUE WANG

    JIANGNAN UNIVERSITY, CHINA

  • HELAN XU

    JIANGNAN UNIVERSITY, CHINA

  • XIULIANG HOU

    JIANGNAN UNIVERSITY, CHINA

Post Views: 26
Posted in WOOD RESEARCH Volume 70, Number 2, 2025Tagged composite paper, deep eutectic solvent, Ginkgo leaf, kapok fiber, willow catkin

Search for a Keyword

Cite This Article

MA, Z., ZHOU, M., WANG, Y., WANG, Q., XU, H., HOU, X. (2025): Preparation of Eco-Friendly Composite Paper with Ginkgo leaf and Bio-based fibers. : Wood Research 70 (2), 273-285 pp., available at: doi.org/10.37763/wr.1336-4561/70.2.273285

Articles in this Release

  • PREPARATION OF ECO-FRIENDLY COMPOSITE PAPER WITH GINKGO LEAF AND BIO-BASED…

  • PULPING AND PAPERMAKING POTENTIAL OF ACACIA AULACOCARPA BENTH WOOD IN…

  • EFFECT OF ALKALINE TREATMENT ON MORPHOLOGY AND BIODEGRADATION OF BAGASSE…

  • THE EFFECT OF UV ABSORBERS ON THE LIGHTFASTNESS OF DYED…

  • STUDY ON THE HYDROTHERMAL TREATMENT OF KILN-DRIED TIMBER OF RED…

  • EFFECT OF SUPERCRITICAL CO2 DEHYDRATION TREATMENT ON THE JUGLANS MANDSHURICA

  • CHEMICAL CHANGES DURING WOOD CUTTING

  • Short notes. INFLUENCE OF WOOD ANATOMY ON THE DISTRIBUTION OF…

Copyright © 2025 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)