Preparation The Rose-like hydrophobic surface of wood based materials by soft lithography

Authors

  • Zeyu Zhang

    Beihua University, China

  • Bingru Shao

    Beihua University, China

  • Fapeng Wang

    Beihua University, China

  • Jiuyin Pang

    Beihua University, China

  • Ling Su

    Beihua University, China

Post Views: 100
Posted in WOOD RESEARCH Volume 66, Number 2, 2021Tagged Hydrophobic wood, polystyrene, polyvinyl alcohol, rose petals, soft lithography

Search for a Keyword

Cite This Article

ZHANG, Z., SHAO, B., WANG, F., PANG, J. & SU, L. (2021): Preparation The Rose-like hydrophobic surface of wood based materials by soft lithography. In: Wood Research 66 (2), 211-220 pp., available at: doi.org/10.37763/wr.1336-4561/66.2.211220

Articles in this Release

  • Development and validation of an analytical method for condensed tannin…

  • Tensile properties of surface modified bamboo slices coated with epoxy…

  • Comparative analysis of static and dynamic MoE of pannĂ³nia poplar…

  • Influence of the environmental pollution on the distribution and polymerization…

  • Preparation The Rose-like hydrophobic surface of wood based materials by…

  • Elimination of adhesive impurities of the recovered paper in flotation…

  • Mechanical properties of polish-grown Pinus Sylvestris L. structural sawn timber…

  • Changes in gross calorific value of thermally treated scots pine…

  • Effects of different flame retardant treatments on the combustibility of…

  • Physical and mechanical characterization of Planchonella Pachycarpa wood species for…

  • Porosity and pore size distribution of recent and ancient buried…

  • Influence of kraft lignin on the properties of rubber composites

  • Internal cause analysis of damage of wooden components in danxia…

  • Bending characteristics of laminated wood composites constructed with black pine…

  • Numerical study on effects of tenon sizes on withdrawal load…

Copyright © 2025 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)