Research on shear performance of components connected by beech and self-tapping screw composite dowels
This study examined the properties of components connected by beech and self-tapping screw composite dowels (group C). As a contrast, the components connected by beech dowels and self-tapping screws individually were tested. The test results indicated that the properties of the components connected by beech dowels (group B) were better than those connected by self-tapping screws (group S), except the ductility coefficient, final displacement, and energy consumption. On the other hand, the main failure modes of groups B and S were the broken beech dowel and the bent self-tapping screw, respectively. For group C, two peak values could be found which were larger than the maximum load of groups B and S, respectively. The properties of group C were better than those of groups B and S, except that the final displacement and energy consumption were located between those of groups B and S. Meanwhile, the linear equation in two unknowns have be found between groups B, S and C.