Effects of wax and dimethyl silicone oil mixed impregnation on dimensional stability of two hardwoods

In this experiment, cocobolo (Dalbergia retusa Hesml.) and African padauk (Pterocarpus soyauxii) specimen were selected before treating with wax, wax + 20% dimethyl silicone oil, wax + 40% dimethyl silicone oil at 120°C for 3 h and 6 h respectively. The weight gain percentage (WPG), radial swelling coefficients (RS), tangential swelling coefficients (TS), chemical composition and strength of hydroxyl groups were investigated. The results indicated that three factors affect dimensional stability, including the impregnation time, tree species and ratio of wax /dimethyl silicone oil. The degree of a melioration in the dimensional stability increase as the impregnation time increase from 3h to 6h. The effect of the impregnation on the dimensional stability of the African padauk was better than that of the cocobolo. Wax+ 40% dimethylsilicone oil was the optimal condition in this study. Wax and dimethylsilicone oil mixed impregnation can improve the dimensional stability to a certain extent, which provides a new idea for the wood modification.

Effects of light thermal treatments on the color, hygroscopity and dimensional stability of wood

Ailanthus wood (Ailanthus desf.) was thermally treated at three different low temperatures (140, 160, 180°C) for 2 and 4 h in order to investigate the effects on wood color, hygroscopity and dimensional stability. Results indicate that mass loss increased following the treatments, while equilibrium moisture content decreased from 11.86% to 9.88% for the 180°C and 4 h treatment. Moreover, improvements in the dimension stability were observed for post-treatment samples. The thermal treatment induced color changes in the Ailanthus wood, with a significant reduction in the lightness, yet the redness and yellowness exhibited minimal changes. FITR spectra of the thermally treated wood suggest that the heat treatment resulted in the deacetylation of hemicellulose. These results help to conclude that thermal treating temperature under 160°C can improve wood dimensional stability and maintain original color.