VARIATION IN BASIC DENSITY AND TRANSVERSE SHRINKAGE AMONG SIX EUCALYPTUS CLONES PLANTED IN VIETNAM

This study examined clonal and radial variation in basic density (BD) and transverse shrinkage among six Eucalyptus clones grown under uniform conditions in north-central Vietnam. A total of 30 ramets were sampled, and 196 small clear specimens were prepared from positions near the pith and the bark. Partial and total shrinkage in tangential (Tn, T) and radial (Rn, R) directions were determined following ISO 13061-13:2017. Basic density (BD) ranged from 0.39 to 0.50 g/cm³ and increased consistently from pith to bark. Tangential shrinkage (Tn: 4.45–5.83%; T: 5.64–6.85%) showed greater variation among clones than radial shrinkage (Rn: 2.95–3.32%; R: 3.89–4.72%). Clone U1427 showed the highest BD while also presenting the lowest shrinkage values, suggesting excellent dimensional stability and considerable potential for utilization in solid wood and lumber production in northern Vietnam.

Mechanical Properties of PF and MUF Bonded Juvenile Hybrid Eucalyptus Plywoods Produced in Ghana

To obtain the mechanical properties of plywood produced from six yearold hybrid Eucalyptus in Ghana was the objective of this research. The samples for the experiment were prepared and tested according to GS EN 326-1, GS EN 310, GS EN 314-1, and GS EN 314 -2. The data obtained were analysed using the factorial ANOVA analysis. The mean results obtained for the various treatments were MOE (6520 – 7638 N/mm2), MOR (53.29 – 60.56 N/mm2, shear strength (2.47 – 5.51 N/mm2), failure (72 -90%) and density (725 – 748 kg/m3). The orientation of the surface veneer caused variations among treatments whiles the adhesives PF and MUF largely did not cause any variations among treatments. This study has proven that it is possible to produce sufficiently strong and resistant plywood from the juvenile wood of eucalyptus.

Evaluation of the characteristics of Eucalyptus pellita and acacia hybrid superior clones selected from breeding program in Indonesia as materials for pulp and papermaking

This study evaluates the characteristics of superior clones of Eucalyptus pellita and Acacia hybrid (Acacia mangium × A. auriculiformis) aged six years selected from a breeding program in Indonesia as materials for pulp and papermaking. Height, diameter, and wood density differed significantly between species and among the clones, with respective mean values 21.6 m, 12.57 cm, and 657 kg.m-3 for E. pellita and 19.5 m, 24.83 cm, and 567 kg.m-3 for Acacia hybrid. Most fiber morphologies were significantly different between species. Cellulose and lignin differed significantly only among Acacia hybrid clones. The mean value of screened pulp yield Acacia hybrid (52.50%) was higher than that of E. pellita (50.31%). Kappa number and brightness were significantly different between species and among E. pellita clones. Some correlations of growth and wood properties showed a better relationship to pulp properties. Handsheet properties varied between species, and some clones showed an outstanding one.

Wood quality of six eucalyptus clones planted in northern Mato Grosso State, Brazil

The present work had the goal of assessing the wood quality through physical-mechanical properties of six 5-year old eucalyptus clones currently planted in northern Mato Grosso State, Brazil. The following clones were assessed, five of them Eucalyptus grandis x Eucalyptus urophylla hybrids and one a clone of Eucalyptus camaldulensis. The physical-mechanical properties were basic density as a function of tree height; pith-to-bark direction; linear, tangential and radial shrinkage; and anisotropic coefficient, longitudinal and parallel compression and static bending strengths; and hardness. Eucalyptus grandis x Eucalyptus urophylla hybrids showed the best wood quality. Concerning to mechanical results, the clones reached intermediate values of strength and rigidity, qualifying them for use in structural applications with less stringent requirements. Considering that all the clones had juvenile wood, the mechanical properties were satisfactory, making the clones suitable for industrial uses.