Aging of Wooden Components in Ancient Timber Structures. Fire Risk and Smoke-Heat Hazards

Based on the aging characteristics of wooden components, this study adopted artificial accelerated aging and fire propagation apparatus (FPA) to examine how aging affects the combustion behaviour, fire risk, and smoke-heat hazards of pine wood commonly used in ancient structures. Wood specimens with dimensions (100×100×10 mm and 300×100×10 mm) matching fire performance tests were prepared, and artificial accelerated photoaging treatment was conducted to obtain aged samples with 0, 60 and 120 aging cycles in accordance with the accelerated aging test protocol for wood materials. The results indicate that pine combustion involves three distinct thermal stages: pyrolysis, smouldering, and flaming, with critical high-risk transition points identified. Aging intensified fire risk and related hazards across all stages, particularly accelerating flame spread on vertical components.

Influence of an age and damage of the oak wood on its fire risk

The aim of this work is to study the effects of different ages and damage of the oak wood (Quercus petraea Mattusch) in relation to its flash point temperature and ignition temperature, as well as on determination of the ratio of changes in extractives, cellulose and lignin, in the heat loaded samples of 5 – years old oak wood, 160 – years old oak wood, and also 160 – years old oak wood degraded by wood-destroying insects and fungi. The results of the analyses showed that the flash point temperatures were in the range of 357.52°C – 360.63°C.The ignition temperatures were at interval of 398.93°C – 414.92°C. The time to reach the ignition point was at the interval between 344 and 365 seconds. Under the thermal loading of oak wood, there comes to the significant changes, especially in the surface layers. These are, in addition to colour changes, demonstrated the chemical changes of the main components of wood and extractives. Increasing the temperature, there increases also the content of the substances extractable with ethanol and toluene. Increase in their amount is mainly due to the lignin, but partially also due to the polysaccharides decomposition products.

Impact of electrical cables embedded into oriented strand board on critical heat flux

The paper deals with the research of electrical cables embedded in surface grooves of OSBs and its impact on the critical heat flux. An OSB type 3 board (structural board for use in dry or humid environments) and an electrical cable with fire reaction class B2ca have been investigated. Four different configurations of grooves were investigated. The first configuration consisted of an OSB without grooves (control sample). The second configuration consisted of an OSB with a single groove in the centre in which the electrical cable was mounted. In the third and fourth configurations, there were three and five grooves, respectively in which the electrical cables were mounted (the width of the grooves and the spacing between them was 9 mm). The critical heat flux was calculated from the ignition times at five different heat fluxes (30, 35, 40, 45 and 50 kW.m-2) by using a cone calorimeter. The obtained data showed that the OSB without grooves (first configuration) shows the lowest critical heat flux (8.6 kW.m-2) and the lowest standard deviation of ± 0.5 kW.m-2 (lower ignition resistance) compared to the other configurations (critical heat flux in the range from 9 to 10 kW.m-2 and standard deviation from 3.1 to 3.2 kW.m-2).