Quality of beech, birch and oak wood from stands growing on post-agricultural lands

Authors

  • Karol Tomczak

    Poznan University of Life Sciences, Poznań, Poland

  • Przemysław Mania

    Poznań University of Life Sciences, Poland

  • Arkadiusz Tomczak

    Poznań University of Life Sciences

Post Views: 268
Posted in WOOD RESEARCH Volume 68, Number 2, 2023Tagged agricultural land, Betula pendula, Fagus sylvatica, Farmland, Quercus spp., wood production, wood quality

Search for a Keyword

Cite This Article

TOMCZAK, K., MANIA, P. & TOMCZAK, A. (2023): Quality of beech, birch and oak wood from stands growing on post-agricultural lands. In: Wood Research 68 (2), 279-292 pp., available at: doi.org/10.37763/wr.1336-4561/68.2.279292

Articles in this Release

  • Evolution and distribution of shakes in larch logs during air…

  • Discoloration of oak veneer induced by metal ions

  • Chemical composition and potential uses of Leucaena leucocephala stem bark

  • Water retention of beech shavings heat-treated at lower temperatures

  • A synergic effect of water-based acrylic resin with boric acid…

  • Quality of beech, birch and oak wood from stands growing…

  • Response surface optimization based on freeze-thaw cycle pretreatment of poplar…

  • Prediction of efficacy of deacidification process

  • Fixation of dye-type red and blue ink handwriting on aged…

  • Determination of mode I fracture properties of European spruce

  • Effects of Pyrolysis process on products yield of plywood from…

  • Volatile organic compounds and metals adsorption capacity of wood bark-based…

  • Optimization of the manufacturing of Metasequoia-based three-layer structure parquet flooring…

  • Model construction and microwave preheating experiments using fiberboard

  • Short notes: First report of the lignivorous fungus Paecilomyces maximus…

Copyright © 2025 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)