EVALUATION OF SELECTED MECHANICAL AND PHYSICAL PROPERTIES OF PARTICLEBOARDS CONTAINING WASTE PLASTICS

This article is focused on the research of particleboards (PB) composed of wood particles from spruce logs and recycled crushed plastic granulates. Crushed plastic granulates sized from 1.0 to 4.0 mm were obtained from worn automobiles by recycling, specifically painted and unpainted bumpers. The proportion of plastic granulate in the particleboards represented 10%, 15%, and 20% of the total weight of the composites. In the production of PB, urea-formaldehyde resin and paraffin emulsion were used as a binder and ammonium nitrate was used as a hardener. The aim of the article was to compare the selected properties of PB containing plastic filler with pure PB. Mechanical properties (tensile and bending strength), and physical properties (water absorption and thickness swelling) were evaluated according to EN 319, EN 310 and EN 317. Based on the results, it can be stated that the bending strength and physical properties of PB containing plastic filler were significantly better compared to pure PB. On the contrary, the tensile strength values were lower in most cases

The influence of chosen factors of a circular saw blade on the noise level in the process of cross cutting wood

Research was focused on evaluation of a circular saw blade tooth spacing on maximum equivalent noise level LAeq in the process of cross cutting wood. There were used circular saw blades with uniform tooth spacing and a full body and non-uniform tooth spacing with dilatation gaps. The measurements were done on the measuring device which was designed at the Department of Environmental and Forest Technology where it has been modernised. For research, testing samples of three wood species i.e. spruce (Picea abies), pine (Pinus sylvestris) and beech (Fagus sylvatica) were used. In the cutting process, two feeding speeds were set up with the same revolutions of circular saw blades and for more precise statistical significance; every measurement was repeated several times. At the research, there was found out that the circular saw blade with uniform tooth spacing has lower equivalent noise level at smaller feeding speed and cutting soft wood species. The circular saw blade with non-uniform tooth spacing has lower equivalent noise level at higher feeding speed.

Impact of the selected factors on the cutting force when using a chainsaw

The paper deals with the calculation and analysis of cutting force and input power when crosscut sawing with a chainsaw. For obtaining and evaluating the results, we have used empirical relationships and the values of appropriate coefficients given by the literature. After the evaluation we have gained the theoretical knowledge of the impact of a tree species and its moisture on cutting force intensity and input power. Tree species have a strong influence on cutting force; the harder the tree species is, the greater cutting force is required. Input cutting power is calculated from the cutting force that is why the impact of a tree species on input power is as big as on cutting force. It has been confirmed that the cutting force and cutting input power are affected by wood moisture content, as well.