Effect of heat treatment on bamboo fiber morphology crystallinity and mechanical properties

This study aimed to investigate the fiber morphology, crystalline structure and mechanical properties of heat-treated bamboo. Moso bamboo was treated by superheated steam at 120, 140, 160, and 180ºC. Fiber morphology and crystalline structure of heat-treated Moso bamboo were researched by transmission electron microscope and X-ray diffraction. The mechanical properties of heat-treated bamboo were tested in the paper. The result showed that the relative crystallinity and length-width ratio of heat-treated bamboo were increased with increased temperature. The elastic modulus of bamboo was increased as the temperature rose from 120 to 140ºC. and then decreased with higher temperature, which was associated with the increase of the crystallinity.

Adsorption and fixation of soluble fire retardancy in Populus russkii and Cunninghamia lanceolata

Flame retardant treatment is a common method of wood preservation. However, the factory usually uses the same approach to all the wood, but lack of targeted so as to cause waste. This study used poplar and Chinese fir as the species investigated. These species were dipped with boron-nitrogen-phosphorus (B-P) fire retardant. The influences on material loading of processing method, concentration of fire retardant, and drying method were investigated. The contents of B and P were tested by inductively coupled plasma optical emission spectrometry (ICP-OES), after distilled water washing and ultrasonic washing. The results showed that the volume loading increased with the concentration of fire retardant. Freeze-drying can noticeably improve the volume loading, and the impact of the drying method was more notable on poplar than on Chinese fir. The fixation effect of the B and P in poplar was lower by ultrasonic washing than that was by distilled water washing. The fixation effect was opposite in the Chinese fir. Vacuum process was more suitable for the poplar (hardwood), and vacuum-pressure process was
more suitable for the Chinese fir (soft wood).