Study on permeability of Cunninghamia Lanceolata based on steam treatment and freeze treatment

In order to improve the permeability of Cunninghamia lanceolata, the weight gain rate of C. lanceolata was taken as index. The effect of time, temperature and water content on the weight gain rate of impregnated wood was analyzed by frozen and steaming treatment. By comparing the weight gain rate under different modification methods, the optimal modification process was determined. The results indicate that the optimum parameters of C. lanceolata were saturated water content (-25°C and 8 h) at this time, the three-day gain rate of silica sol impregnated at normal temperature and pressure was 15.058%. After C. lanceolata is pre-treated by superheated steam, the weight gain rate of C. lanceolata, which in oven-dried specimen (120°C and 3 h) contents was the highest, at this time, the three-day gain rate of silica sol impregnated at normal temperature and pressure was 15.291%. By comparing the results of pre-freezing with the results of superheated steam treatment of C. lanceolata, the latter will increase the permeability of C. lanceolata better. Therefore superheated steam treatment should be chosen as an effective method for the pretreatment.

Short Note: Non-standard test method for glue line shear strength

The relevant standards for glueline shear strength testing were summarized and analyzed in this paper. Depending on these existing test standards, the resulting stress in glueline is not pure shear stress, but a combination of shear and normal stresses. In order to overcome this deficiency, a symmetrical structure was proposed for making samples. Some comparative testing was accomplished by using these symmetrical samples, the results showed that the normal stress could be avoided during testing. These results were also confirmed by finite element method (FEM), the simulation results showed that the shear stress in glueline was uniform.