Physico-acoustic characteristics of spruce and larche wood

This study deals with non-destructive measurement of wood, i.e. physico-acoustic characteristics (density, dynamic modulus of elasticity, acoustical constant, speed of sound propagation in material and logarithmic dumping decrement). We used two species spruce and larch for measurements. We took wood from two main areas: from Slovakian higher latitudes and from Russia – Siberian areas. Spruce is the main species for the boards of musical instruments and we tried to find another species to replace this one. We measured physico-acoustic properties by two devices: The ultra-sonic tester and device “MEARFA” based on searching correct frequency for each sample. The results show that spruce for top instruments has acoustic constant approx. 12 m4∙kg-1∙s-1 and the “best” value for larch was approx. 10 m4∙kg-1∙s-1. If we compare the methods of measurement of the sound velocity through samples the results for ultrasonic testing are much higher than those provided by resonance-dynamic method. The article also describes differences between physico-acoustical characteristics of sap wood and heart wood, and differences between species.

Dependence of spruce wood resonance properties on its chemical composition

Nowadays there are no reasoned scientific data on inter relation of resonant properties of spruce-tree wood and its chemical composition. Thus the purpose of the study was to reveal the features of sonorous spruce in view of the content of basic organic substances in their timber. 20 model trees at the age of 180-190 years were selected as material for studies in taiga woods in the north of Kirov region of Russia. Special 0.5 m long blocks were made from each model tree at height of 1.3 m. Standard 20×20×300 mm samples were made from those blocks. Test samples were kept at room dry conditions for 2 years. After that dendro acoustic studies were carried out on them to define acoustic constant in different directions with respect to timber fibers. Further the percentage of cellulose, lignin, extractives and ashes in them was defined applying standard techniques. As a whole the chemical composition of spruce tree resonant wood lies approximately within the same limits as in common wood of the breed given. However significant influence of cellulose on a longitudinal acoustic constant and lignin on a radial constant is revealed. Joint influence of lignin and cellulose on a tangential constant is found out, the influence of lignin in the latter case being dominant. Continuation of fundamental research in this field has great cognitive value for revealing the nature of unique acoustic properties formation in sonorous spruce wood. Such studies acquire special topicality when dealing with outstanding violins as well as the wood kept for many decades in old buildings subject to demolition.