Study on concentrations of acids and alcohols emitted by pinus radiata during high-temperature drying

Authors

  • Jiangyi Chu

    Chinese Academy Of Forestry, China

  • Jinghui Jiang

    Chinese Academy Of Forestry, China

  • Chusheng Qi

    Beijing Forestry University, China

  • Yongdong Zhou

    Chinese Academy Of Forestry, China

Post Views: 101
Posted in WOOD RESEARCH Volume 66, Number 3, 2021Tagged emission of acid and methanol, high-temperature drying, Lumber, moisture content, Pinus radiata, relative humidity

Search for a Keyword

Cite This Article

CHU, J., JIANG, J., QI, CH. & ZHOU, Y. (2021): Study on concentrations of acids and alcohols emitted by pinus radiata during high-temperature drying. In: Wood Research 66 (3), 427-436 pp., available at: doi.org/10.37763/wr.1336-4561/66.3.427436

Articles in this Release

  • Effects of polymer additives on some mechanical and physical properties…

  • Study and analysis on sound absorbing and noise reducing performance…

  • Effect of different pre-treatments on the permeability of glue-laminated bamboo

  • Characteristic features of the oil-heat treated woods from tropical fast…

  • Eco-design: Impacts of bleaching chemicals and varnishes on the amount…

  • Fiber morphology and physical properties of branch and stem wood…

  • Characterization of aromatic fiberboard

  • A comparative study on the physical and mechanical properties of…

  • Study on concentrations of acids and alcohols emitted by pinus…

  • Effects of hot pressing parameters on the properties of hardboards…

  • Biosocial diversity of scots pine (pinus sylvestris l.) in a…

  • Data mining and its impact on marketing communication – case:…

  • Effect of different wood dowels on mechanical properties of triangular…

  • Axial compression testing of bamboo plywood-encased thin-walled steel tube/stone dust…

  • Effect of addition of deinked pulp to bleached kraft pulp…

Copyright © 2025 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)