Dynamic relationship between mechanical properties and chemical composition distribution of wood cell walls

Author

  • Enhua Xi

    Shandong Agricultural University, College of Forestry, Tai’an, China

    Institute of Wood Science of Shandong Province, Tai’an, China

Post Views: 435
Posted in WOOD RESEARCH Volume 63, Number 2, 2018Tagged chemical composition, growing season, mechanical properties, wood cell wall

Search for a Keyword

Cite This Article

XI, E. (2018): Dynamic relationship between mechanical properties and chemical composition distribution of wood cell walls. In: Wood Research 63 (2), ISSN 1336-4561, VUPC (SDVU), 179-192 pp.

Articles in this Release

  • Dynamic relationship between mechanical properties and chemical composition distribution of…

  • Chemical characteristics of Eucalyptus pellita with heart rot

  • Indoor fungal destroyers of wooden materials – their identification in…

  • Dynamic and damping properties of novel bio-composites using the hammer…

  • Effect of macro characteristics on rolling shear properties of fast-growing…

  • The bending modulus of elasticity of subfossil elm wood

  • Study on thermal insulation and heat transfer properties of wood…

  • Change in the wood moisture dependency on time and drying…

  • Probabilistic approach of the failure of Lovoa trichilioides and Triplochiton…

  • Characteristics of nontoxic bamboo bioboard by melamine and cellulose adhesive

  • Optimization of the clearance angle in industrial disc chipper

  • The synergistic smoke suppression effect of ferric oxide on flame…

  • Determination of viscosity curve and PVT properties for wood-polymer composite

  • Study on continuous cold-pressing technology of engineered wood flooring with…

  • Measuring the surface roughness values of european hop-horn beam (Ostrya…

  • Fabrication of superhydrophobic wood surface with a silica/silicone oil complex…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}