The selected properties of fossil oak wood from medieval burgh in Płońsk

Authors

  • Piotr Mańkowski

    Warsaw University of Life Sciences – SGGW,
    Poland

  • Paweł Kozakiewicz

    Warsaw University of Live Science,
    Poland

  • MICHAŁ DROŻDŻEK

    WARSAW UNIVERSITY OF LIFE SCIENCES, POLAND

Post Views: 318
Posted in WOOD RESEARCH Volume 61, Number 2, 2016Tagged Archaeological oak wood, mechanical and chemical properties of wood, physical

Search for a Keyword

Cite This Article

MANKOWSKI, P., KOZAKIEWICZ, P. & DROZDZEK, M. (2016): The selected properties of fossil oak wood from medieval burgh in Płońsk. In: Wood Research 61 (2), ISSN 1336-4561, VUPC (SDVU), 287-298 pp.

Articles in this Release

  • Microstructure characterization of wood fiber pit adsorbing ultrafine particles emitted…

  • Fungicide efficacy of nanofibre textiles containing chemical preservatives for protection…

  • The adhesion properties of wood preserved with natural preservatives

  • Development of bonding strength of modified birch veneers during adhesive…

  • The effect of pigments and binders on inkjet print quality

  • Effect of heat treatment on bamboo fiber morphology crystallinity and…

  • Results of rheological test on timber trusses

  • Optimization of L-shaped corner dowel joint in pine using finite…

  • Steaming treatment decreases MOE and compression strength of Turkey oak…

  • Improving mechanical and physical properties of particleboard made from vine…

  • Optimization of laser cutting parameters for recombinant bamboo based on…

  • The selected properties of fossil oak wood from medieval burgh…

  • The potential for using corn stalks as a raw material…

  • Mechanical material properties effect on pelletization

  • Analysis of durability and dimensional stability of hydrothermal carbonized wooden…

  • Testing model for assessment of lignocellulose-based pellets

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}