Measuring the electric resistance of air drying thick red pine and larch timber

Authors

  • Hong Shuang Du

    Beihua University, China

  • Chengyuan Li

    Beihua University, China

  • Chun Won Kang

    Jeonbuk National University, Republic of Korea

Post Views: 224
Posted in WOOD RESEARCH Volume 67, Number 5, 2022Tagged air drying, electric resistance, Japanese larch (Larix leptolepis G.), Red pine (Pinus densiflora)

Search for a Keyword

Cite This Article

Du, H. S., Li, Ch. & Kang, Ch. W. (2022): Measuring the electric resistance of air drying thick red pine and larch timber. In: Wood Research 67 (5), 866-874 pp., available at: doi.org/10.37763/wr.1336-4561/67.5.866874

Articles in this Release

  • Research on the structure and connections of pits in different…

  • Wood density and annual ring width of pedunculate oak from…

  • The effects of ACQ and water glass on the color…

  • Research on the effect of wood surface cracks on propagation…

  • Impregnation on poplar wood with vegetable oils: Effects on physical…

  • Impact of thermal modification combined with silicon compounds treatment on…

  • Comparative study of particleboards with Hevea brasiliensis waste from different…

  • The effect of a phenol-formaldehyde adhesive reinforcement with nanocellulose on…

  • Densification and effect of compression ratio on mechanical properties of…

  • Influence of vacuum impregnation pressures on the nanomechanical characteristics and…

  • Influence of pumice powder on some properties of phenol-formaldehyde bonded…

  • Evaluation of the characteristics of Eucalyptus pellita and acacia hybrid…

  • Measuring the electric resistance of air drying thick red pine…

  • A deep learning program for predicting sap flow of Larix…

  • Short notes: Can the physical properties of wood samples be…

Copyright © 2025 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)