EXPERIMENTAL AND NUMERICAL INVESTIGATION OF CLT PANELS WITH DIFFERENT ORIENTATIONS OF TRANSVERSE LAYERS

Authors

  • MARIJA TODOROVIĆ

    University of Belgrade, Faculty of Civil Engineering, Belgrade, Serbia

  • IVAN GLIŠOVIĆ

    University of Belgrade, Faculty of Civil Engineering, Belgrade, Serbia

  • NAĐA SIMOVIĆ

    University of Belgrade, Serbia

Post Views: 168
Posted in WOOD RESEARCH Volume 69, Number 4, 2024Tagged CLT, conventional and modified layup, experimental test, FE model

Search for a Keyword

Cite This Article

TODOROVIĆ, M., GLIŠOVIĆ, I., SIMOVIĆ, N. (2024): Experimental and Numerical Investigation of Clt Panels with Different Orientations of Transverse Layers.In: Wood Research 69 (4), 625 – 637 pp., available at: doi.org/10.37763/wr.1336-4561/69.4.625637

Articles in this Release

  • INNOVATIVE CELLULOSE ADSORBER TO INCREASE TREE PROTECTION AGAINST HARMFUL EFFECTS…

  • DESIGN AND ANALYSES OF HYBRID FACADE PANELS CREATED WITH TRANSPARENT…

  • EXPERIMENTAL STUDY ON FLEXURAL BEHAVIOR OF RED MERANTI (SHOREA SPP.)…

  • COMPARISON OF TWO METHOD FOR ISOLATION OF FIBRILLATED CELLULOSE FROM…

  • INFLUENCE OF PARTICULATE MIXTURE CONTAINING STABILISED WOOD ON LONG-TERM BEHAVIOUR…

  • LIGNOCELLULOSIC WASTE OF FURFURAL PRODUCTION FROM BAGASSE AS NON-FOOD FILLER…

  • THE EFFECT OF COLORANTS ON THE DEGRADATION PERFORMANCE OF WOOD…

  • ENZYMATIC HYDROLYSIS OF STEAM EXPLODED STRAW WITH THE ADDITION OF…

  • THE ATTENUATION CHARACTERISTICS OF DIFFERENT FREQUENCY COMPONENTS OF ACOUSTIC EMISSION…

  • MECHANICAL STRENGTH CHARACTERIZATION OF THREE LESSER-UTILISED TIMBER SPECIES IN GHANA

  • EXPERIMENTAL AND NUMERICAL INVESTIGATION OF CLT PANELS WITH DIFFERENT ORIENTATIONS…

  • THE EFFECT OF WEATHERING ON SURFACE CHARACTERISTICS OF CHEMICALLY MODIFIED…

  • ANISOTROPIC VELOCITY MODEL AND ENERGY ATTENUATION CHARACTERISTICS OF ACOUSTIC EMISSION…

  • INFLUENCE OF TEMPERATURE AND PRESSURE ON SUPERCRITICAL CO2 DEWATERING OF…

  • RADIAL AND AMONGCLONAL VARIATIONS OF TRANSVERSE SHRINKAGE AND BASIC DENSITY…

  • MAPPING WOOD DENSITY VARIATION USING QGIS: AN INNOVATIVE APPROACH FOR…

Copyright © 2025 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)