Adsorption and fixation of soluble fire retardancy in Populus russkii and Cunninghamia lanceolata

Authors

  • Hong Yun

    South China Agricultural University,
    China

  • Kaifu Li

    South China Agricultural University,
    China

  • Chuangshuang Hu

    South China Agricultural University,
    China

  • Dengyun Tu

    South China Agricultural University,
    China

Post Views: 341
Posted in WOOD RESEARCH Volume 62, Number 2, 2017Tagged adsorption, fire retardant, Fixation

Search for a Keyword

Cite This Article

YUN, H., LI, K., HU, CH. & TU, D. (2017): Adsorption and f ixation of soluble f ire retardancy in Populus russkii and Cunninghamia lanceolata. In: Wood Research 62 (2), ISSN 1336-4561, VUPC (SDVU), 253-260 pp.

Articles in this Release

  • Determination of the phenolic extractive content in sweet chestnut (Castanea…

  • Grafting organic-inorganic compound modifier onto wood cell walls for enhanced…

  • Variability of Black locust hardness in relation to different measurement…

  • The impacts analysis of moisture content on mechanical properties of…

  • Physico-acoustic characteristics of spruce and larche wood

  • Tensile-shear strength of layered wood reinforced by carbon materials

  • Adsorption and fixation of soluble fire retardancy in Populus russkii…

  • Adsorption of 4-chlorophenol from aqueous solution on activated carbons derived…

  • Possibilities of removing condensate from a heat recovery unit utilizable…

  • Effect of wood modifiers on the physical properties of fast-…

  • Comparison of measured and calculated values of cutting forces in…

  • An examination of the tool life and surface quality during…

  • Torrefaction of lamellar panels made of oak and spruce wood…

  • Short note. Addition of propylamine as formaldehyde scavenger for urea…

  • Short note. Physical and mechanical properties of Paulownia tomentosa wood…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}