Alterations in the anatomy and chemical structure of archaeological wood from a tomb of northern china due to different fungal rots

Authors

  • Yihang Zhou

    Peking University.
    P.R. China

  • Kai Wang

    Northeast Forestry University, China

  • Xueqi Chen

    Peking University,
    P.R. China

  • Dongbo Hu

    Peking University,
    P.R. China

Post Views: 340
Posted in WOOD RESEARCH Volume 65, Number 5, 2020Tagged 13C NMR, Archaeological wood, FT-IR, microscopy, wood decay, XPS

Search for a Keyword

Cite This Article

ZHOU, Y., WANG, K., CHEN, X. & HU, D. (2020): Alterations in the anatomy and chemical structure of archaeological wood from a tomb of northern china due to different fungal rots. In: Wood Research 65 (5), 757-770 pp., available at: doi.org/10.37763/wr.1336-4561/65.5.757770

Articles in this Release

  • Promotion effect of nano-SiO2 on hygroscopicity, leaching resistance and thermal…

  • Strength and stiffness of mechanically jointed CLT panels loaded by…

  • Effect of lamina thickness on flexural performance and creep behavior…

  • Addition of sugarcane bagasse for the production of particleboards bonded…

  • In situ hydrothermal synthesis of MnO2 nanowires/wood derived activated carbon…

  • Effect of pressing temperatures on bonding properties of sucrose-citric acid…

  • Alterations in the anatomy and chemical structure of archaeological wood…

  • Determination of maximum torque during carpentry waste comminution

  • A study on noise levels of machinery used in lumber…

  • Study of nano colloidal silica sol based protectant on the…

  • Wood degrading mushrooms potentially strong towards laccase biosynthesis in Pakistan

  • Testing and analysis of hemlock cross laminated timber

  • Extraction of betulin from the birch bark balance at pulp…

  • A multi-stage cascade use of wood composite boards

  • Cork from Quercus suber L.: Forest certification system for sustainable…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}