Analysis of diagnostic methods for detecting the presence of gloeophyllum spp

Authors

  • Roman Fojtík

    Všb-Technical University of Ostrava, Faculty of Civil Engineering Department
    of Building Structures, Ostrava, Czech Republic

  • Kateřina Dědková

    Všb-Technical University of Ostrava, Centre for Advanced and Innovative Technologies, Ostrava, Czech Republic

Post Views: 311
Posted in WOOD RESEARCH Volume 63, Number 3, 2018Tagged bridges, diagnostics, Wood, wood decaying fungi

Search for a Keyword

Cite This Article

FOJTIK, R. & DEDKOVA, K. (2018): Analysis of diagnostic methods for detecting the presence of gloeophyllum spp. In: Wood Research 63 (3), ISSN 1336-4561, VUPC (SDVU), 479-486 pp.

Articles in this Release

  • Antibacterial efficiency of silver and zinc-oxide nanoparticles in acrylate coating…

  • Effect of hygroscopicity of fire retardant on hygroscopicity of fire…

  • The effect of the relaxation time on the mechanical properties…

  • Visual simulation on dynamic accumulation of the differentiating xylem cells

  • The strength and termite resistance characteristics of fiberboards produced from…

  • Degradation features of archaeological wood surface to deep inside a…

  • Waste agglomerated wood materials as a secondary raw material for…

  • Determination of leaching features of wood surfaces colored by eco-friendly…

  • Analysis of cutting performance in high density fiberboard milling by…

  • Organosolv pulping of Calotropis procera by mono ethanol amine

  • Analysis of diagnostic methods for detecting the presence of gloeophyllum…

  • Technique to improve paint utilizing efficiency of wooden board during…

  • Wood quality of Paraserianthes falcataria L. nielsen syn wood from…

  • Optimal design of stretchers positions of mortise and tenon joint…

  • Hydrophobic properties of wood traeted with propolis-silane formulations

  • Cultural and creative product design based on biology characteristics of…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}