Assessment of Smartphone-Based 3D Scanning as an Alternative to Xylometry for Measuring Small, Irregular Wood Pieces Generated during Harvesting

This study evaluates the applicability of smartphone-based 3D scanning for measuring small, irregular wood pieces generated by felling notches in windthrown Norway spruce (Picea abies L.) stands. A total of 114 notch pieces were measured using both a conventional xylometric method and a smartphone-based 3D scanning method. The volumes obtained by the two methods showed an exceptionally strong correlation (r = 0.9993) and excellent absolute agreement (ICC = 0.9992). The Bland–Altman analysis indicated 95% relative limits of agreement of −15.36% to +25.20%, together with a significant proportional bias. The total notch loss index was 0.186% using xylometry and 0.184% using 3D scanning. The regression analysis showed that notch height was the only significant predictor of the loss index. The results indicate that smartphone-based 3D scanning is a promising method for estimating the volume of small and irregular wood pieces, although its interchangeability with xylometry requires predefined acceptable measurement limits.