Effects of Vegetable Oil Type and Impregnation Method on the Uptake, Leaching Resistance, and Dimensional Stability of Wood

Vegetable oils and their derivatives (VODs) were evaluated as sustainable wood treatments to improve the water resistance and dimensional stability of Japanese larch (JAC), Douglas-fir, western hemlock, and yellow poplar under saline-water exposure. Specimens were treated with castor oil (CAO), hydrogenated castor oil (HCO), soybean oil (SBO), and waste cooking oil (WCO) using coating, immersion, vacuum (VAC), and vacuum-pressure (VAC-PRES) methods. VOD uptake varied with its type, and treatment method. Leaching resistance followed the order HCO > SBO > CAO > WCO, whereas all treatments, except those using WCO, significantly improved dimensional stability compared with untreated controls. JAC specimens treated with HCO by VAC impregnation exhibited the lowest VOD concentration in leachates and the greatest dimensional stability. Overall, VOD impregnation enhanced wood performance under saline-water exposure, with VAC impregnation using HCO identified as the most effective treatment. These findings highlight the potential of HCO-treated wood for exterior and marine applications.

Graphical Assignment of Equivalent Narrow-Cut Depths and Rotational Stiffnesses for Finite-Length Tie-Beam Section Reductions

A graphical procedure relates finite-length tie-beam section reductions to the measured and calculated narrow-cut response of one three-frame timber roof segment. Fifteen numerical cases combine reduction lengths of 100–300 mm with remaining heights of 20–60 mm. Local displacement and midspan deflection give separate equivalent cut-depth readings; an adopted common depth is then used to read approximate rotational stiffnesses k1 and k2 from the adjusted measured and calculated narrow-cut series, respectively. For a 200 mm long reduction with 40 mm remaining height, the local and midspan readings are 4.89 and 5.06 cm, with an adopted depth of 5.0 cm. Agreement with the narrow-cut curves and the subsequent spring-model response are assessed separately. Both displacements yield in-range depths for 12 of the 15 cases; three exceed the calculated response range. Experimental testing covered the narrow cuts.

Evaluating the Applicability of Proteinaceous Interfacial Binders in Polylactic Acid-Lignocellulosic Filler Composites

This study evaluated the applicability of protein‑based interfacial binders in the production of polylactic acid (PLA)-lignocellulosic filler composites. The composites were fabricated by blending PLA with radiata pine (RDP), hardwood scrub (MIX), cypress bark powder (CYP-B) powder as fillers, hydrogenated castor oil (HCO) as a dimensional stabilizer, and black soldier fly (BSF) powder, or a freeze-dried proteinaceous adhesive resin (PAR) powder formulated from BSF hydrolyzates as interfacial binders. Composites fabricated with PLA, CYP-B, PAR-1, and HCO showed superior impact/bending strengths and lower moisture absorption rate compared to RDP- or MIX-filled composites. A formulation of 50 wt% PLA, 40 wt% CYP‑B, 5 wt% PAR, and 5 wt% HCO showed the best overall performance, outperforming composites using maleic anhydride as a conventional synthetic interfacial binder. Overall, PAR is a promising substitute for expensive, hazardous synthetic binders, and CYP‑B is a viable waste‑valorization filler with environmental and health benefits.

Assessment of Smartphone-Based 3D Scanning as an Alternative to Xylometry for Measuring Small, Irregular Wood Pieces Generated during Harvesting

This study evaluates the applicability of smartphone-based 3D scanning for measuring small, irregular wood pieces generated by felling notches in windthrown Norway spruce (Picea abies L.) stands. A total of 114 notch pieces were measured using both a conventional xylometric method and a smartphone-based 3D scanning method. The volumes obtained by the two methods showed an exceptionally strong correlation (r = 0.9993) and excellent absolute agreement (ICC = 0.9992). The Bland–Altman analysis indicated 95% relative limits of agreement of −15.36% to +25.20%, together with a significant proportional bias. The total notch loss index was 0.186% using xylometry and 0.184% using 3D scanning. The regression analysis showed that notch height was the only significant predictor of the loss index. The results indicate that smartphone-based 3D scanning is a promising method for estimating the volume of small and irregular wood pieces, although its interchangeability with xylometry requires predefined acceptable measurement limits.

Effect of Freeze–Thaw Cycle on the Screw-Holding Strength of Plywood

In this study, five-layered plywood boards were produced with poplar, beech, and eucalyptus rotary peeled veneer. One control group and three experimental group test samples were prepared from the produced boards. The experimental group test samples were subjected to 2, 4, and 6 freeze–thaw cycles according to TS EN 321. The density, moisture content, and screw-holding strength of each test sample were determined. Screw-holding tests were performed according to the principles specified in TS EN 13446. In the tests, a screw was applied perpendicular to the surface of the test sample. The poplar plywood had the lowest screw holding strength, with the highest found in the beech plywood. The effects of 4 and 6 freeze–thaw cycles on the screw-holding strength were statistically significant. A strong relationship was found between the screw-holding strength and density of the plywood.

Experimental Assessment of Reinforcement Anchorage in CLT Grooves under Tensile Loading

Sixteen tensile tests examine reinforcement anchorage in cross-laminated timber (CLT) grooves for hybrid-floor continuity connections. Two concrete-groove widths, two epoxy systems and headed-bar pockets with and without screws are compared using peak forces, apparent quasi-linear stiffnesses, force–elongation curves and observed damage. Companion bar tests provide reference forces. Concrete grooves with basic widths of 45 and 55 mm reached mean peak forces of 24.80 and 21.71 kN, respectively, with continued force transfer after cracking. Mean peak forces were 46.71 kN for XEPOX FLUID and 51.89 kN for HIT–RE 500 V4. The Hilti specimens showed plastic deformation of the reinforcement, whereas the XEPOX curves formed two response groups. Two screws increased the headed-pocket peak force from 26.08 to 41.50 kN and altered cracking. HIT–RE 500 V4 and XEPOX FLUID exhibited mean apparent quasi-linear stiffnesses of 8.6 and 7.7 kN/mm, respectively.

Analysis of Structural Characteristics of Bacterial Nanocellulose Synthesized Using Beechwood Hydrolysate

In this study, a comprehensive structural analysis to increase yield, optimize cultivation parameters, and evaluate bacterial nanocellulose (BNC) organization using two types of media was conducted. Cultivation of Komagataeibacter xylinus (K. xylinus) DSM 46591 was performed in an alternative beechwood hydrolysate medium (BH) and the standard Hestrin–Schramm medium (HS) over a period of 72–432 h. High–performance liquid chromatography (HPLC) confirmed the successful extraction of glucose, xylose, and associated compounds from the wood. Fourier–transform infrared spectroscopy (FTIR) revealed visible changes in supramolecular structure in BH, resulting in a 12.8% decrease in the lateral order index (LOI: 0.748 → 0.652) and a simultaneous increase in the hydrogen bond index (HBI: 0.997 → 1.111) in comparison with HS. X–ray diffraction (XRD) showed that BH promotes the synthesis of a combination of cellulose triclinic (Iα) and monoclinic (Iβ) with a high crystallinity index (CI = 86%), while sterically limiting lateral crystallite growth (the crystallite sizes (CS) of the (002) crystallographic plane were 6.1–6.5 nm for BH vs. 6.7 nm for HS). Scanning electron microscopy (SEM) confirmed that, in BH, this resulted in a reticulated, interconnected three–dimensional nanofibrillar matrix with preserved capillary porosity. In contrast, the HS samples showed pore clogging, denser fibre packing, and layer stacking.