Graphical Assignment of Equivalent Narrow-Cut Depths and Rotational Stiffnesses for Finite-Length Tie-Beam Section Reductions

A graphical procedure relates finite-length tie-beam section reductions to the measured and calculated narrow-cut response of one three-frame timber roof segment. Fifteen numerical cases combine reduction lengths of 100–300 mm with remaining heights of 20–60 mm. Local displacement and midspan deflection give separate equivalent cut-depth readings; an adopted common depth is then used to read approximate rotational stiffnesses k1 and k2 from the adjusted measured and calculated narrow-cut series, respectively. For a 200 mm long reduction with 40 mm remaining height, the local and midspan readings are 4.89 and 5.06 cm, with an adopted depth of 5.0 cm. Agreement with the narrow-cut curves and the subsequent spring-model response are assessed separately. Both displacements yield in-range depths for 12 of the 15 cases; three exceed the calculated response range. Experimental testing covered the narrow cuts.

Experimental Assessment of Reinforcement Anchorage in CLT Grooves under Tensile Loading

Sixteen tensile tests examine reinforcement anchorage in cross-laminated timber (CLT) grooves for hybrid-floor continuity connections. Two concrete-groove widths, two epoxy systems and headed-bar pockets with and without screws are compared using peak forces, apparent quasi-linear stiffnesses, force–elongation curves and observed damage. Companion bar tests provide reference forces. Concrete grooves with basic widths of 45 and 55 mm reached mean peak forces of 24.80 and 21.71 kN, respectively, with continued force transfer after cracking. Mean peak forces were 46.71 kN for XEPOX FLUID and 51.89 kN for HIT–RE 500 V4. The Hilti specimens showed plastic deformation of the reinforcement, whereas the XEPOX curves formed two response groups. Two screws increased the headed-pocket peak force from 26.08 to 41.50 kN and altered cracking. HIT–RE 500 V4 and XEPOX FLUID exhibited mean apparent quasi-linear stiffnesses of 8.6 and 7.7 kN/mm, respectively.

Experimental Investigation of Load Redistribution in a Historic-Type Timber Roof Segment Under Progressive Tie-Beam Weakening

This study examines how progressive loss of tie-beam stiffness redistributes deformation demand and internal force within an experimentally verified historic timber roof segment. A three-frame laboratory model was evaluated by close-range photogrammetry, inductive displacement sensing, post-test bending tests, and finite-element modelling. The measurements revealed clear frame-to-frame stiffness asymmetry, a distinct pre-cut settlement phase under sustained load, and accelerated deformation once the residual tie-beam section was substantially reduced. A refined model using member-specific elastic parameters reproduced the global loading response more accurately than a uniform-stiffness model. The damaged zone could also be represented by an equivalent rotational spring, although the fitted spring values remained response-dependent. The results indicate that lathing acted as a temporary redundancy path after severe weakening and that a nearly hinged residual section was not mechanically equivalent to a fully severed member within the tested configuration.

THE EXPERIMENTAL INVESTIGATION OF A MODEL OF A HISTORICAL-TYPE TIMBER ROOF SEGMENT UNDER PROGRESSIVE TIE-BEAM WEAKENING

This paper reports on an experimental study of a model of a historical timber roof segment subjected to progressive weakening of the central tie beam. A three-frame specimen was tested under controlled loading, short-term sustained full load, and sequential cutting of the middle tie beam. Close-range photogrammetry was combined with inductive displacement sensors and conventional control measurements. The study examined the agreement of optical and contact measurements, redistribution of displacement demand to the adjacent frames, and the temporary residual stability provided by lathing after complete failure of the middle tie beam. Across the tie-beam midspans, the mean absolute difference between inductive and paired optical measurements ranged from 0.07 to 0.40 mm, with a maximum point-wise deviation of 1.39 mm. After complete failure, additional settlement of the two intact frames reached 4.28 and 3.97 mm relative to the pre-cut full-load state, indicating longitudinal redistribution through the lathing.

DETERMINATION OF FLEXURAL STRENGTH AND YOUNG’S MODULUS OF ELASTICITY OF ACTIVELY BENT WOOD

The article focuses on the experimental verification of wooden laths with a cross-section of 10 mm x 40 mm which were selected for active bending. The laths are made of pine wood and are 2 m in length. The research includes experimental measurements to determine the limit deformations achieved by bending the wood without chemical treatment, by applying compressive force to an originally straight beam, causing it to buckle and further deform. Ten bending tests of beams were performed, and from the same pieces, 21 tests were conducted using the four-point bending test to determine the flexural strength, and 30 tests to determine the global modulus of elasticity

Experimental tests of timber connections with glued-in rods in bending

The article deals with research of joints with glued-in threaded rods. The introduction provides a brief presentation of the issue. The first part focuses on axially loaded glued-in threaded rods. The second part explains the behaviour of joints with glued-in rods loaded by bending moment. Theoretical analysis was performed on models based on the finite element method. Verification of theoretical results was realized by practical experiments. Tensile tests were carried out on timber blocks with glued-in bars to verify the depth of affixing. Furthermore, the resistance in bending was confirmed on actual beams with glued-in bars in the middle of the span. Results and the follow-up work are summarized in the conclusion.