Skip to content
Wood Research
Menu
  • Home
  • Author guidelines
  • Journal Issues
  • Contact

Steam-pressing mechanism of low density magnesia-bonded wood-wool panel

Authors

  • Chengshuo Sun

    Nanjing Forestry University, China

  • Kang Zhou

    Nanjing Forestry University,
    China

  • Zirui Ren

    Nanjing Forestry University, China

  • Yutang Chen

    Nanjing Forestry University, China

  • Bin Na

    Nanjing Forestry University,
    China

Post Views: 698
Posted in WOOD RESEARCH Volume 67, Number 3, 2022Tagged Magnesite, scanning electron microscope, steam-pressing mechanism, wood-wool panel, X-ray diffraction

Search for a Keyword

Cite This Article

SUN, CH., ZHOU, K. & NA, B. (2022): Steam-pressing mechanism of low density magnesia-bonded wood-wool panel. In: Wood Research 67 (3), 437-446 pp., available at: doi.org/10.37763/wr.1336-4561/67.3.437446

Articles in this Release

  • Impact of heat treatment on the surface color and glossiness…

  • Effect of UV radiation on change in color of steamed…

  • Why the sound-absorbing performance of heartwood and sapwood differs in…

  • Comprehensive evaluation of hawthorn wood characteristics in relation to soil…

  • Relationship between cell lumen area and lignin content of alkaline-treated…

  • Timbre harmonic of selected hardwood species

  • Effects of fire retardants on mechanical properties and water resistance…

  • Modelling of steel to timber joint exposed to fire

  • Steam-pressing mechanism of low density magnesia-bonded wood-wool panel

  • Deformation behavior of circular saw blades with different body structures…

  • Modelling of post–consumer wood sorting and manipulation: Computational conception and…

  • A micro-graph retrieval system for coniferous woods using multiple methods

  • Bamboo defect classification based on improved transformer network

  • Short notes: A research on the application of industrial by-product…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}