Study on cold/warm sensation of materials used in desktop of furniture

Authors

  • Wen-Gang Hu

    Nanjing Forestry University, China

  • Na Liu

    Nanjing Forestry University, China

  • Lu Xu

    Nanjing Forestry University, China

  • Huiyuan Guan

    Nanjing Forestry University, China

Post Views: 488
Posted in WOOD RESEARCH Volume 65, Number 3, 2020Tagged cold/warm sensation, Desktop, forearm, furniture

Search for a Keyword

Cite This Article

HU, W., LIU, N., XU, L. & GUAN, H. (2020): Study on cold/warm sensation of materials used in desktop of furniture. In: Wood Research 65 (3), 497-506 pp., available at: doi.org/10.37763/wr.1336-4561/65.3.497506

Articles in this Release

  • The influence of thermal modification on the resistance to water…

  • Resonance and time-of-flight methods for evaluating the modulus of elasticity…

  • Effect of the metallization treatment on the surface properties of…

  • A study on suitability of some wood species for landscape…

  • Comparison of selected properties of natural aged wood and contemporary…

  • Characterization of new mutant Eucommia ulmoides constituents in the discoloration…

  • Influence of gaseous plasma treatment on functional properties of coated…

  • Effect of agricultural residue fibers on newsprint strength properties

  • Blending impact of hardwood pulps with softwood pulp on tissue…

  • Gene pool of Scots pine (Pinus sylvestris L.) under reforestation…

  • Heat-induced inkless eco-printing inspired by paper discoloration: A review

  • Effect of the fabric reinforcement of structural holes in wood…

  • Study on cold/warm sensation of materials used in desktop of…

  • Economical design of timber-concrete composite beams

  • An experimental study on sustainability of historical wooden buildings exposed…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}