The Comparison of the Effect of UV Irradiation and the Combined Effect of UV Irradiation and Water Leaching on the Color of Grey Poplar

A series of grey poplar (Populus x canescens) samples was irradiated by strong ultraviolet (UV) light emitter mercury lamp, while another series of specimens were treated with the combination of UV irradiation and water leaching. The total duration of UV irradiation for both series of specimens was 20 days. The colour parameters (CIE L*, a*, b*) were measured and evaluated after both UV irradiation and water leaching. Due to the 20 days of UV irradiation, the initial redness value of sapwood increased 2.69 times, while leaching reduced this factor to 1.77. In case of heartwood, the initial redness value increased 1.34-fold due to the 20-day UV exposure, while the leaching reduced this factor to 1.14. These multiplier values are 2.07 and 1.44 for the yellowness of sapwood, as well as 1.57 and 1.29 for the yellowness of heartwood. The leaching partly removed the yellow and red chromophore molecules generated by the UV irradiation. The samples were slightly lighter after water leaching

INFRARED SPECTRUM CHANGE OF UV IRRADIATED AND NATURAL WOOD SAMPLES DURING 12 YEARS OF STORAGE IN TOTAL DARKNESS

The stability of the surface of UV-irradiated wood samples was investigated after 12 years of storage in total darkness at room temperature. The investigated specimens were earlywood and latewood of Scots pine sapwood, earlywood and latewood of spruce, earlywood of ash, beech and hybrid poplar. The thin (1 mm tick) samples contained only earlywood or latewood, and the tangential surfaces were used for infrared spectrum measurement. For comparison, the non-irradiated natural surface (back side) of the specimens was used for infrared spectrum measurement. Natural wood surfaces were stable during the storage. Only ether linkages in hemicelluloses showed minor degradation at 1175 cm-1 wavenumber. Lignin molecules remained stable during the 12-year storage period on both UV irradiated and non-irradiated side of the specimens. In contrast, UV irradiated samples suffered alterations during the 12 years of thermal treatment at low temperature (20-25°C). Hemicelluloses in photodegraded surface layers underwent thermal degradation and oxidation processes, generating new carbonyl groups. Extractives also presented absorption increase in the conjugated carbonyl region

Colour change of photodegraded spruce wood by water leaching

Spruce samples (Picea abies Karst.) were irradiated by strong ultraviolet (UV) light emitter mercury lamp and another series of specimens were treated with the combination of UV radiation and water leaching. The total duration of UV radiation for both series of specimens was 50 days. The colour parameters (CIE L*, a*, b*) were measured and evaluated after both UV radiation and water leaching. The increase of redness value was two times greater than the yellowness increase based on the initial value at the end of 50 days treatment. The leaching partly removed the yellow and red chromophore molecules generated by the UV radiation. The samples become slightly lighter after water leaching. The leached samples increased slightly more in yellowness and redness during the first 4-6 days of UV radiation than those of the dry series. The change of surface roughness of the specimens was monitored by diffuse reflectance infrared spectroscopy, because the change of roughness alters the light scattering properties of the surface. The roughness of the samples increased during the UV irradiation, and the tendency of roughness change mirrored that of yellowness change. The leaching reduced the roughness value in all examined cases. Good correlation was found between the hue angle and the lightness in both dry UV treatment and combined UV treatment and water leaching.

Effect of water leaching on photodegraded poplar wood monitored by IR spectroscopy

Poplar (Populus x euramericana cv. pannonia) samples were irradiated using ultraviolet light emitter mercury lamp. Other series of specimens were treated with the combination of UV radiation and water leaching. The total duration of UV radiation for both series of specimens was 20 days. The total duration of water leaching was 10 days. One cycle of the combined treatment consisted of 2-day UV radiation followed by one day water leaching. The IR measurement was carried out after both UV radiation and water leaching to monitor both effects separately. Lignin degradation of water leached samples was found to be greater than that of the solely UV treated samples. The guaiacyl and the syringyl lignin showed similar degradation properties. The unconjugated carbonyl groups generated by the photodegradation proved to be the most sensitive chemical components to leaching. As a consequence of photodegradation, two absorption bands of unconjugated carbonyl groups were grown up at 1715 and 1759 cm-1 wavenumbers. The band at 1759 cm-1 was much more sensitive to water leaching than the band at 1715 cm-1. Ten days of water leaching was long enough to remove all unconjugated carbonyls generated by the photodegradation. The water was able to leach out carbonyl groups (absorbing at 1745 cm-1) originally presented in poplar wood as well.