Colour change of photodegraded spruce wood by water leaching

Authors

  • ANTAL KÁNNÁR

    UNIVERSITY OF SOPRON, HUNGARY

  • LASZLO TOLVAJ

    UNIVERSITY OF SOPRON, HUNGARY

  • Endre Magoss

    University of Sopron, Simonyi Karoly Faculty of Engineering, Wood Sciences and Applied Arts, Sopron, Hungary

Post Views: 404
Posted in WOOD RESEARCH Volume 63, Number 6, 2018Tagged colour change, leaching by water, photodegradation, spruce

Search for a Keyword

Cite This Article

KANNAR, A., TOLVAJ, L. & MAGOSS, E. (2018): Colour change of photodegraded spruce wood by water leaching. In: Wood Research 63 (6), ISSN 1336-4561, VUPC (SDVU), 935-946 pp.

Articles in this Release

  • Impact of different radiation forms on beech wood discolouration

  • Colour change of photodegraded spruce wood by water leaching

  • Characterizations and properties of torrefied Quercus variabilis cork

  • Testing of wood physical properties in oak species (Quercus robur…

  • Treatability indices of some plant species of fabaceae in Nigeria

  • Seismic evaluation of wood frame construction based on nail connection…

  • Resistance of various materials and coatings used in wood constructions…

  • Performance of activated carbon obtained from pine wood and determination…

  • Tackiness reducing of the stickies surfaces by inorganic agents and…

  • Thermopressed binderless fiberboards from wheat straw by adding black liquor

  • Determination of some properties of Scotch pine (Pinus sylvestris L.)…

  • Pelletization of invasive Reynoutria japonica with spruce sawdust for energy…

  • Moisture dependent elastic constants of particleboard layers by ultrasound and…

  • Contrastive analysis of screw withdrawal resistance between bamboo oriented strand…

  • Impact of cationic polyacrylamide for a new kind of pulp…

  • Analysis of composite action of various mass timber structural panels…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}