SHORT NOTE. THERMAL CHARACTERISTICS OF SENGON WOOD DRYING USING INFRARED AND COMBINED INFRARED-HOT AIR METHODS

Authors

  • YEFRI CHAN

    SEBELAS MARET UNIVERSITY, INDONESIA
    DARMA PERSADA UNIVERSITY, INDONESIA

  • DWI ARIES HIMAWANTO

    SEBELAS MARET UNIVERSITY, INDONESIA

  • BUDI KRISTIAWAN

    SEBELAS MARET UNIVERSITY, INDONESIA

  • INDRI YANINGSIH

    SEBELAS MARET UNIVERSITY, INDONESIA

Post Views: 787
Posted in WOOD RESEARCH Volume 69, Number 1, 2024Tagged drying, infrared, infrared-hot air, sengon wood, temperature

Search for a Keyword

Cite This Article

CHAN, Y., HIMAWANTO, D. A., KRISTIAWAN, B., YANINGSIH, I. (2024): Thermal characteristics of Sengon wood drying using infrared and combined infrared-hot air methods. In: Wood Research 69 (1), 01-08 pp., available at: doi.org/10.37763/wr.1336-4561/69.1.0108

Articles in this Release

  • THE OPTIMAL IMPREGNATION AMOUNTS OF FLAME-RETARDANT FOR KOREAN LARCH AND…

  • EVALUATION OF SELECTED MECHANICAL AND PHYSICAL PROPERTIES OF PARTICLEBOARDS CONTAINING…

  • STUDY ON PREPARATION TECHNOLOGY OF HIGH-QUALITY BIOMASS FUEL PELLETS USING…

  • STUDY ON THE MOST EFFECTIVE COMBINATION OF FLAME RETARDANT AND…

  • EVALUATION OF DYNAMIC AND STATIC MODULI OF ELASTICITY OF HYBRID…

  • THIN LIGNOCELLULOSIC LINERS BASED OF SPRUCE SHAVINGS

  • CHARACTERIZATION OF EXTRACTIVE COMPOSITION IN THE WOOD AND BARK OF…

  • INFLUENCE OF SITES ON THE PHYSICAL AND MECHANICAL PROPERTIES OF…

  • CLIMATE CHANGE MITIGATION THROUGH CARBON STORAGE AND PRODUCT SUBSTITUTION IN…

  • MODIFIED STARCHES AS A MEAN OF INCREASING THE DRY STRENGTH…

  • OPTIMAL DESIGN OF THE TRADITIONAL CHINESE WOOD FURNITURE JOINT BASED…

  • VARIABILITY OF ANATOMICAL AND MORPHOLOGICAL TRAITS OF PINUS NIGRA AND…

  • SOME PHYSICAL AND MECHANICAL PROPERTIES OF COCONUT PALM (COCOS NUCIFERA)…

  • PREPARATION AND PERFORMANCE OF ANTI MILDEW GLUED LAMINATED BAMBOO

  • SHORT NOTE. THERMAL CHARACTERISTICS OF SENGON WOOD DRYING USING INFRARED…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}