WR2020 04: 01-15 WR 202004

Contents:

download


1. HUIMIN ZHANG, KAI TU, QIANDONG HOU, HUI LIN, QUAN LI:

The physiological and biochemical mechanisms of Cinnamomum camphora xylem extracts inhibit wood-decay fungi. 531
doi.org/10.37763/wr.1336-4561/65.4.531542


2. LAÉRCIO SERENINI JR., RAFAEL RODOLFO DE MELO, DIEGO MARTINS STANGERLIN, ALEXANDRE SANTOS PIMENTA:

Wood quality of six eucalyptus clones planted in northern Mato Grosso State, Brazil. 543
doi.org/10.37763/wr.1336-4561/65.4.543554


3. ENDRE MAGOSS, SÁNDOR TATAI, ZSOLT MOLNÁR, INGRID FUCHS:

A calibration method of the laser triangular measuring system to evaluate wood surface roughness. 555
doi.org/10.37763/wr.1336-4561/65.4.555564


4. JIANHUA LYU, WEIHUI HUANG, MING CHEN, XIANWEI LI, SHILIN ZHONG, SIYUAN CHEN, JIULONG XIE:

Analysis of tracheid morphological characteristics, annual rings width and latewood rate of Cupressus funebris in relation to climate factors. 565
doi.org/10.37763/wr.1336-4561/65.4.565578


5. ANDREJ PAŽITNÝ, ALBERT RUSS, ŠTEFAN BOHÁČEK, MONIKA STANKOVSKÁ, VLADIMÍR IHNÁT, ŠTEFAN ŠUTÝ:

Effect of steam explosion on enzymatic hydrolysis of various parts of poplar tree. 579
doi.org/10.37763/wr.1336-4561/65.4.579590


6. ZHU LIU, LIANG WEN, XUAN WANG, YAOLI ZHANG, LIPING CAI:

Leachability of ACQ-D after three different preservative treatments. 591
doi.org/10.37763/wr.1336-4561/65.4.591604


7. KATARÍNA DÚBRAVSKÁ, ĽUDMILA TEREŇOVÁ, JAROSLAVA ŠTEFKOVÁ:

CLT construction performance under thermal loading. 605
doi.org/10.37763/wr.1336-4561/65.4.605614


8. HONG YUN, CHUANGSHUANG HU, JIN GU, YILIN HAN, XIAOJING HU:

Study on the permeation and fixation of ACQ-C in poplar. 615
doi.org/10.37763/wr.1336-4561/65.4.615622


9. EHSAN YOUSEFI, MOHAMMADREZA DEHGHANI FIROOZABADI, OMID GHAFFARZADEH, VLADIMÍR KUŇA:

Investigation of urea usage in soda pulping of Populus deltoides. 623
doi.org/10.37763/wr.1336-4561/65.4.623632


10. HUICHUAN JIANG, QUANJI LU, GUANJUN LI, MIN LI, JIANING LI:

Effect of heat treatment on the surface color of rubber wood (Hevea brasiliensis). 633
doi.org/10.37763/wr.1336-4561/65.4.633644


11. ROMAN FOJTÍK, VIKTOR DUBOVSKÝ, KATEŘINA KOZLOVÁ, LENKA KUBÍNCOVÁ:

Prestress losses in spruce timber. 645
doi.org/10.37763/wr.1336-4561/65.4.645652


12. WŁODZIMIERZ SZEWCZYK, MARIA BIEŃKOWSKA:

Effect of corrugated board structure on mechanical properties. 653
doi.org/10.37763/wr.1336-4561/65.4.653662


13. QUAN LI, HUIMIN ZHANG, HONGGUANG YAN, WENYU QI, JINGUO LIN, JIQING LI:

Emission of volatile camphor compounds from Cinnamomum camphora wood. 663
doi.org/10.37763/wr.1336-4561/65.4.663674


14. ONUR ULKER, MERCAN HADDAD DERAFSHI:

Evaluation of corner joint strength of composite panels bonded with modified starch. 675
doi.org/10.37763/wr.1336-4561/65.4.675686


15. ANDREAS TREU, ERIK LARNØY:

Short note: The impact of glue-lines on the protective effect of a low- pulsed electric field in wood. 687
doi.org/10.37763/wr.1336-4561/65.4.687692